Thông tư 83/2002/TT-BTC
Văn bản rất dài (1,9 MB). Trang này hiện phần đầu để tải nhanh.
Mục lục · 0 Điều
OFFICIAL GAZETTE
No. 53 (25-10-2002)
THE MINISTRIES
THE MINISTRY OF FINANCE
CIRCULAR No. 83/2002/TT-BTC OF SEPTEMBER 25, 2002 PRESCRIBING THE REGIME OF COLLECTION, REMITTANCE AND MANAGEMENT OF THE USE OF STANDARDIZATION, MEASUREMENT AND QUALITY CONTROL CHARGES AND FEES
Pursuant to the October 6, 1999 Measurement Ordinance and the December 24, 1999 Goods Quality Ordinance;
Pursuant to the August 28, 2001 Charge and Fee Ordinance and the Government�s Decree No. 57/2002/ND-CP of June 3, 2002 detailing the implementation of the Charge and Fee Ordinance;
The Ministry of Finance hereby prescribes the regime of collection, remittance and management of the use of standardization, measurement and quality control charges and fees, as follows:
A. CHARGES AND FEES FOR STATE MANAGEMENT OVER STANDARDIZATION, MEASUREMENT AND QUALITY CONTROL
I. PAYERS AND COLLECTION LEVELS
1. Vietnamese and foreign organizations and individuals shall have to pay charges and fees for State management over standardization, measurement and quality control under the provisions of this Circular when the State management agencies in charge of standardization, measurement and quality control or authorized agencies carry out the registration, testing and State inspection of product and goods quality as well as the checking of measuring equipment for them according to current law provisions.
2. The rates of standardization, measurement and quality control charges and fees are specified in the tables of charge and fee rates, issued together with this Circular, including:
- The table in Appendix No. 1: The rates of charges, including the charge for testing of product or goods quality; the charge for State inspection of product or goods quality; and the charge for checking of measuring devices.
- The table in Appendix No. 2: The rates of the charges for registration and granting of standardization, measurement and quality control certificates
3. Standardization, measurement and quality control charges and fees specified in this Circular shall be collected in Vietnam dong (VND).
II. ORGANIZATION OF THE COLLECTION, REMITTANCE, USE MANAGEMENT
1. The standardization, measurement and quality control agencies that register, test, inspect product and goods quality and/or check measuring devices according to law provisions shall have to:
a/ Organize the collection and remittance of standardization, measurement and quality control charges and fees strictly according to the provisions of this Circular. Announce (or post up publicly) the rates of standardization, measurement and quality control charges and fees at the head offices of the charge- and/or fee-collecting agencies. When collecting charges and fees, issue charge or fee receipts (of a type issued by the Ministry of Finance) to the payers.
b/ Open accounting books to monitor the collected and remitted amounts and used charge and fee amounts strictly according to the current legislation on accounting and statistics.
c/ Register, declare, and remit standardization, measurement and quality control charges and fees under the guidance of the tax offices of the localities where they are headquartered.
d/ Make payment and settlement for charge and fee receipts as well as settlement of the charge and fee collection and remittance with the direct managing tax offices according to the regime of management of receipts and stamps prescribed by the Ministry of Finance.
2. The collected amounts of standardization, measurement and quality control charges and fees shall be managed and used as follows:
a/ Before remitting the collected charge and fee amounts into the State budget, the standardization, measurement and quality control agencies may retain a portion in percentage (%) of the total collected charge and fee amounts. Concretely:
- 85% (eighty five per cent) of the charge for testing of product or goods quality, the charge for State inspection of product and goods quality, and the charge for checking of measuring devices.
- 10% (ten per cent) of the fee for registration and granting of standardization, measurement and quality control certificates.
b/ They remit into the State budget the remainder (the total amount of actually collected charges and fees minus the amounts retained according to the percentages specified at Item a of this point, including:
- 15% (fifteen per cent) of the charge for testing of product or goods quality; the charge for State inspection of product and goods quality, and the charge for checking of measuring devices.
- 90% (ninety per cent) of the fee for registration and granting of standardization, measurement and quality control certificates.
3. The standardization, measurement and quality control agencies may spend the charge and fee amounts retained according to the percentages specified at Item a, Point 2 of this Section on the collection of standardization, measurement and quality control charges and fees according to the following particular spending contents:
a/ Payment of salaries, remunerations, allowances and expenses for working in hazardous conditions (including labor safety expenses, if any) to the charge and/or fee-collecting laborers, salary- and wage-based contributions belonging to the employers� responsibility according to the prescribed regime. Where the units receive funding from the State budget to pay salaries to their officials and employees on official payroll, they shall be only allowed to pay remunerations according to the prescribed regime to laborers hired from the outside to collect charges and fees.
b/ Payments for services purchased from the outside to serve the charge and fee collection, such as purchase of office supplies, electricity, water, telephone, information and communication, working-trip allowances (travel, accommodation, sojourn allowance�), printing (purchase) of forms, permits and other prints according to the current spending criteria and norms.
c/ Expenses for meetings, seminars, professional training and fostering, propaganda and advertising in service of the charge and fee collection.
d/ Expenses for regular repair, overhaul of assets, machinery and equipment in direct service of the charge and fee collection.
e/ Expenses for purchase of supplies, raw materials, equipment, working instruments and other expenses in service of the charge and fee collection according to the estimates already approved by competent authorities.
f/ Payment of prescribed yearly dues to international standardization, measurement and quality control organizations that Vietnam has joined, which have not yet been funded by the State budget.
g/ Deductions for the reward and welfare funds for officials and employees involved in the charge and fee collection. The deduction level for setting up these two funds must not exceed the annual average of three months� actually-paid salary per person, if the collected amount is higher than that of the previous year, or of two months� actually-paid salary if the collected amount is equal to or lower than that of the previous year.
The standardization, measurement and quality control agencies shall have to manage and use the retained charge amounts for the above-said purposes and with valid vouchers, and to annually settle the revenues and expenditures that have actually arise. After they effect the settlement according to the prescribed regime, if they have not yet spent all the retained amounts, they may carry forward the unspent amounts to the subsequent year for continued spending according to the prescribed regime.
4. Procedures for declaration and remittance into the State budget of the collected amounts of standardization, measurement and quality control charges and fees are prescribed as follows:
- The standardization, measurement and quality control agencies that collect charges and/or fees shall make and submit to the direct managing tax offices within the first 5 days of the subsequent month monthly declarations on the collected charge and/or fee amounts, the retained charge and/or fee amounts and the monthly charge and/or fee amounts remittable into the State budget and submit the declaration forms to and shall take responsibility for the accuracy of their declarations. Where no fee or charge is collected in the month, they must still make and submit declaration forms to the tax offices.
- On the basis of declaration forms, the standardization, measurement and quality control agencies shall remit the remittable charge and fee amounts into the State budget. The deadline for remitting the previous month�s amounts into the State budget is the 15th day of the current month at the latest (into the corresponding chapter, category and clause, item 045, sub-item 04 of the current State budget classification) at the State treasuries of the places where the standardization, measurement and quality control agencies are headquartered. The charge and fee amounts collected by the centrally-run agencies and remitted into the State budget shall be channeled into the central budget; the charge and fee amounts collected by locally-run agencies and remitted into the State budget shall be channeled into the local budgets.
- Upon receiving the charge and fee declaration forms of the standardization, measurement and quality control agencies, the tax offices shall check and compare them with the receipts already issued and the receipts used so as to determine the collected charge and fee amounts, the amounts to be retained and the amounts remittable into the State budget in the period, then notify the standardization, measurement and quality control agencies of the amounts they must remit into the State budget.
- The standardization, measurement and quality control agencies shall compare the to be-remitted charge and fee amounts as notified by the tax offices with the charge and fee amounts actually remitted into the State budget in the period, if they have not yet remitted them fully, they shall have to remit the deficient amounts into the State budget; if they have remitted them in excess, the over-remitted amounts shall be subtracted from the amounts to be remitted into the State budget in the subsequent period.
5. Making and execution of charge and fee revenue and expenditure estimates:
a/ Annually, on the basis of the rates of standardization, measurement and quality control charges and fees, the spending contents guided in this Circular as well as the current financial expenditure regime, the standardization, measurement and quality control agencies shall make revenue and expenditure estimates of standardization, measurement and quality control charges and fees according to the current State budget classification and send them to their managing agencies for consideration, approval and synthesization before sending them to the same-level finance offices competent to approve them.
b/ On the basis of the annual revenue and expenditure estimates already approved by competent authorities, the standardization, measurement and quality control agencies shall make detailed quarterly revenue and expenditure estimates according to the current State budget classification and send them to their managing agencies and the State treasuries where they have transactions as well as the same-level finance offices as a basis for revenue and expenditure control.
6. Final settlement of charge and fee revenues and expenditures:
a/ The standardization, measurement and quality control agencies shall have to open accounting books to record, account and settle charge and fee revenues and expenditures under the Finance Minister�s Decision No. 999/TC/QD/CDKT of November 2, 1996 issuing the administrative and non-business accounting system and regime; to effect the settlement of receipts of charges and fees already collected and remitted into the State budget; to submit the annual final settlement reports on the collected and remitted standardization, measurement and quality control charges and fees to the tax offices before the last day of February of the year following the reporting year; and to submit fully the deficient charge and/or fee amounts into the State budget within 10 days after the date of submission of their reports.
b/ The tax offices shall effect the settlement of the collected amounts according to their receipts, the total collected amounts, the retained amounts and the amounts remittable into the State budget. The finance offices and the tax offices shall settle the expenditures from the standardization, measurement and quality control charges and fee amounts that the units are permit to retain under the provisions at Point 3, Section II, Part A of this Circular.
c/ The superior managing agencies shall have to check and certify the settlement of the collected and spent amounts of standardization, measurement and quality control charges and fees of their subordinate standardization, measurement and quality control agencies, sum up and incorporate them into their annual final settlement reports and send such reports to the finance offices for evaluation and issuance of notices of approval of the settlement together with the settlement of the superior management agencies according to the provisions of the current State Budget Law.
B. OTHER REVENUES
The standardization, measurement and quality control agencies that earn revenues other than those charges and fees belonging to the State budget specified in Part A of this Circular (such as those collected from the provision of scientific and technical services�) shall be obliged to:
1. Fix the collection levels on the principles of full retrieval of capital within a reasonable time and compatibility with the payers� capability to make contributions as agreed upon.
2. Abide by the law-prescribed invoice and voucher regime. Where the provided services are of a value lower than the level at which invoices must not be made and the customers request no invoices, the list thereof must be made as prescribed.
3. To open accounting books to monitor and account separately expenses and turnovers of other revenues stated in this part (apart from those charges and fees belonging to the State budget) under the current law provisions on accounting and statistics.
4. To pay value added tax, enterprise income tax and other payable amounts (if any) according to current law provisions; the remainder shall be managed and used under the provisions of the Government�s Decree No. 10/2002/ND-CP of January 16, 2002 and the Finance Ministry�s Circular No. 25/2002/TT-BTC of March 21, 2002 guiding the financial regime applicable to non-business units having revenues and other relevant documents.
C. ORGANIZATION OF IMPLEMENTATION
1. This Circular takes effect 15 days after its signing. All provisions on the collection, remittance and use of charges and fees for testing, measurement and other standardization, measurement and quality control activities in Inter-Ministerial Circular No. 65/TT-LB of August 19, 1995 of the Ministry of Finance and the Ministry of Science, Technology and Environment and the regime of collection of fees for testing of measuring devices prescribed in the Finance Ministry�s Circular No. 120/1998/TT/BTC of August 27, 1998 are hereby annulled.
2. The State management agencies in charge of standardization, measurement and quality control shall collect, remit and use charges and fees in the standardization, measurement and quality control domain according to the provisions of this Circular.
3. If any problems arise in the course of implementation, the agencies, organizations and individuals should promptly report them to the Ministry of Finance for study and additional guidance.
For the Minister of Finance
Vice Minister
TRUONG CHI TRUNG
APPENDIX 1 TABLE (CHARGES)
I. RATES OF THE CHARGE FOR TESTING
THE MECHANICAL FIELD
|
Ordinal number |
Product names - criteria |
Quantity |
Testing methods |
Duration - days |
Unit price - VND1,000 |
Notes |
|
1 |
Mechanicality (not including expenses for working and preparation for large or complicated samples) |
|||||
|
1.1 |
Tension test |
|||||
|
a. |
Tension test (metal in round, twisted forms, pipes, tubes, sheets and other shapes, welded joints in these forms, bolts and nuts) |
L > 350 |
Test standards like: |
5 |
d: diameter |
|
|
d � 10 or t � 5 |
a > 150 (for steel sheets) |
TCVN, ASTM, JIS, BS, NF, AS, ISO... |
90 |
L: length |
||
|
b. |
Tension test of metal wires (d � 4 mm) |
3 m |
TCVN 1824: 1993 |
200 |
3 tests/ sample |
|
|
c. |
Tension test of pig-iron cast |
f30 x 0.4m |
TCVN 197: 1985 |
200 |
||
|
d. |
Tension test of steel tubes |
|||||
|
(d � 60 mm) |
1 m |
JIS, TCVN, ASTM |
350 |
|||
|
e. |
Pre-stressed steel cable |
2 m |
ASTM A 370 � 94 |
500 |
||
|
1.2 |
Flexing test |
|||||
|
a |
Flexing test, re-flexing test (metal in round, twisted forms, pipes, tubes, sheets, welded joints in the above-said forms) |
L > 350 |
Testing standards like: |
5 |
||
|
d � 10 or t � 5 |
a > 150 |
TCVN, ASTM, JIS, |
70 |
|||
|
10 < d � 20 or 5 < t � 10 |
(for steel sheets) |
BS, NF, AS, ISO� |
90 |
|||
|
20 < d � 32 or 10 < t � 20 |
140 |
|||||
|
d > 32 or t > 20 |
180 |
|||||
|
b. |
Flexing test of pig iron |
f30 x 0.4m |
ASTM A 438- 80 |
180 |
||
|
1.3 |
Hardness test - Rockwell - Brinell - Vickers - Microscopic - Survey of the hardness of welded samples |
testing standards like TCVN, ASTM, JIS, BS, NF, AS, ISO� |
3 |
70 70 140 200 300 |
||
|
1.4 |
Charpy, Izod impact test |
1 set consisting of 3 samples |
testing standards like TCVN, ASTM, JIS, BS, NF, AS, ISO� |
5 |
including the cost of processing samples up to standards |
|
|
- at room temperature |
300 |
|||||
|
- at room temperature to minus 20oC |
400 |
|||||
|
- at minus 20oC to minus 70 oC |
500 |
|||||
|
1.5 |
Tension test of wires |
3 m |
TCVN 1824:1993 |
3 |
90 |
|
|
1.6 |
Rolling test of wires |
3 m |
TCVN 1825:1993 |
80 |
||
|
1.7 |
Folding test of wires |
3 m |
TCVN 1826:1993 |
3 |
80 |
|
|
1.8 |
Twisting test of wires |
3 m |
TCVN 1827:1993 |
3 |
90 |
|
|
1.9 |
Spreading test of tubes |
1 |
TCVN 5890:1995 ISO 4893: 1986 |
5 |
150
140 |
|
|
1.10 |
Rolling test of tube edge |
1 |
TCVN 1829:1976 |
5 |
150 |
|
|
1.11 |
Spreading test of tube collars |
1 |
TCVN: 5892:1995 ISO 8595: 1986 |
5 |
150 |
|
|
1.12 |
Flat-pressing test of tubes |
1 |
TCVN 1830:1993 |
3 |
120 |
|
|
1.13 |
Flexing test of tubes |
1 |
TCVN 5891:1995 ISO 8491:1986 |
5 |
180 |
|
|
1.14 |
Mechanical test of pig-iron tubes |
3 |
ISO 13 1978 |
5 |
150 |
|
|
1.15 |
Pressure test of tubes |
2m |
ASME BPV |
|||
|
� 60at |
CODE |
As negotiated |
180 |
|||
|
60at � 100 at |
TCVN 1832:1976 |
220 |
||||
|
> 100 at |
I OCT 3845:75 |
300 |
||||
|
1.16 |
Test of steel cables |
L > 300 |
TCVN 5757:1993 ISO 2408:1986 |
4 |
300 |
|
|
1.17 |
Test of electric welding rods (criteria: appearance, adhesion, deviation, immersion strength, moisture, welding technology, chemical composition, mechanicality) |
> 4kg |
TCVN 3909:1994 |
As negotiated |
including the cost of processing samples up to standards |
|
|
* d > 2.5mm |
2,100 |
|||||
|
* d � 2.5mm |
1,800 |
|||||
|
1.18 |
Load test of bolts, screws, studs, nuts |
1 set |
TCVN 1916:1995 |
5 |
100 |
|
|
1.19 |
Test of bolt-tightening momentum |
1 set |
As negotiated |
|||
|
M < 16 |
120 |
|||||
|
M = 16 � 25 |
150 |
|||||
|
M > 25 |
200 |
|||||
|
1.20 |
Test of spring washers (elasticity, flexibility, hardness) |
3 |
TCVN 130:1997 |
5 |
180 |
|
|
1.21 |
Test of welding rods |
2 boxes |
AWS D5.1 |
|||
|
- Demonstration welding and taking photos of welded samples |
500 |
|||||
|
- Tension test of welded metal |
200 |
|||||
|
- Flexing test of welded metal |
170 |
|||||
|
1.22 |
Load test of product details |
1 |
At customers� requests |
not including the expenses for making test fixtures |
||
|
- Under 100 kN |
180 |
|||||
|
- Between 100 kN and 300 kN |
250 |
|||||
|
- From 300 kN and more |
400 |
|||||
|
1.23 |
Measuring geometric sizes |
1 |
Microscopes |
|||
|
- With a precision of up to 0.01mm |
Tools |
50 |
||||
|
- With a precision of up to 0.001 mm |
Multiple-purposes length-measuring machines |
80 |
||||
|
1.24 |
Measuring outer and inner threads |
1 |
80 |
|||
|
1.25 |
Determination of deviations in geometric shapes |
1 |
TCVN 384:1993 |
60 |
||
|
1.26 |
Determination of deviations in correlative positions |
1 |
TCVN 384:1993 |
100 |
||
|
1.27 |
Measuring surface roughness |
1 |
TCVN 2511:1978 |
100 |
||
|
1.28 |
Measuring mirror brightness |
1 |
80 |
|||
|
2 |
Metal organization � coating layer |
7 |
||||
|
2.1 |
Microscopic organization |
1 |
ASM Metals Handbook |
360 |
||
|
2.2 |
Crude organization |
1 |
ASM Metals Handbook |
200 |
||
|
2.3 |
Particle degree |
1 |
JIS G 0551 |
200 |
||
|
2.4 |
Hardenability and decarbonization |
1 |
JIS G 0557 |
200 |
||
|
2.5 |
Measuring the thickness of the coating layer |
1 |
ASM Metals Handbook |
|||
|
- With measuring machines |
60 |
|||||
|
- With metallographic microscope |
150 |
|||||
|
- By weight method |
100 |
|||||
|
2.6 |
Test of coating layer�s adhesiveness |
1 |
TCVN 5408:1991 |
50 |
||
|
2.7 |
Test of coating layer by hoarfrost- spraying method |
1 |
ASTM B 117-94 |
800 |
for one cycle |
|
|
2.8 |
Test of the coating layer�s chemical composition |
2 |
3 QTTN |
|||
|
- Qualitative |
300 |
|||||
|
- Quantitative |
500 |
|||||
|
3 |
Non-destruction test (NDT) |
As negotiated |
(1) |
|||
|
3.1 |
Checking surface defects with Permeability test (PT) |
According to reality |
ASTM E 165-95 |
50/m or 300/m2 |
||
|
3.2 |
Checking surface defects with magnetic test (MT) |
ASTM E 709-95 |
50/m or 300/m2 |
|||
|
3.3 |
Checking defects of welding joints by ultrasonic test (UT) |
ASTM E 164-94 ASME BPV CODE |
70/m |
|||
|
3.4 |
Measuring thickness by ultrasonic test |
According to reality |
ASTM E 797-94 |
6/points |
||
|
3.5 |
Checking with radiation rays (X-ray, � ray) |
According to reality |
ASTM E 142-94 ASME BPV CODE |
100/film |
Film 10 x 250cm |
|
|
4 |
Chemical components of metal |
ASTM E 415-95 |
2 |
One test one sample |
||
|
- 1 element |
1 sample |
90 |
||||
|
- Under 6 elements |
250 |
|||||
|
- Between 6 and 9 elements |
350 |
|||||
|
- From 10 elements and more |
450 |
Notes:
(1) This expense applies to the cases where the test samples are brought by the customers and tested at PTN, not covering expenses for travelling, transportation of equipment, fixtures, preparatory work� as well as other expenses that arise upon field tests.
FIELD: CONSUMER GOODS
|
Ordinal number |
Products names - criteria |
Quantity |
Testing method |
Duration day |
Unit price - VND1,000 |
Notes |
|
1 |
Rubber |
|||||
|
1.1 |
Group 1: Condoms |
1 piece |
||||
|
1.1.1 |
Test of hole - water leakage method |
TCVN 6342-5:1998 |
3 |
5 |
||
|
Test of hole - water leakage method |
" |
ISO 4074-5:1996 |
3 |
5 |
||
|
1.1.2 |
Determination of length |
" |
TCVN 6342-2:1998 |
1 |
2.5 |
|
|
1.1.3 |
Determination of width |
" |
TCVN 6342-3:1998 |
1 |
2.5 |
|
|
1.1.4 |
Determination of volume and explosion pressure (after aging) |
" |
TCVN 6342-7:1998 ISO 4074-7:1996 |
5-9 5-9 |
10 10 |
|
|
1.1.5 |
Determination of volume and explosion pressure (before aging) |
" |
ISO 4074-6:1996 TCVN 6342-6:1998 |
5-9 5-9 |
8 8 |
|
|
1.1.6 |
Weight |
" |
52TC NTTB 01-94 |
5 |
||
|
1.1.7 |
Weight of lubricating oil |
" |
52TC NTTB 01-94 |
20 |
||
|
1.1.8 |
Degree of contamination |
" |
52TC NTTB 01-94 |
5 |
||
|
1.1.9 |
Tensile test |
" |
52TC NTTB 01-94 ISO 4074-9:1980/96 |
10 10 |
||
|
1.1.10 |
Tensile test (after aging) |
" |
52TC NTTB 01-94 ISO 4074-9:1980/96 |
15 15 |
||
|
1.2 |
Group 2: Natural rubber |
0.5kg |
||||
|
1.2.1 |
Plasticity maintenance index |
100g |
TCVN 6092:1995 |
2 |
50 |
|
|
1.2.2 |
Rubber identification |
50g |
ASTM D 3677-90 ISO 4650:1984 |
2 2 |
170 170 |
|
|
1.2.3 |
Initial plasticity |
100g |
TCVN 6092:1995 |
2 |
40 |
|
|
1.2.4 |
Dirt content |
100g |
TCVN 6089:1995 |
2 |
80 |
|
|
1.2.5 |
Content of volatile substances |
100g |
TCVN 6088:1995 |
2 |
40 |
|
|
1.2.6 |
Nitrogen content |
100g |
TCVN 6091:1995 |
3 |
50 |
|
|
1.2.7 |
Ash content |
100g |
TCVN 6087:1995 |
2 |
60 |
|
|
1.3 |
Group 3: Rubber gloves |
|||||
|
1.3.1 |
Water-tightness of sterile disposable rubber gloves used in surgery |
1 piece |
TCVN 6344:1998 |
3 |
5 |
|
|
1.3.2 |
Water-tightness of disposable rubber gloves used in medical examination |
" |
TCVN 6343:1998 |
3 |
5 |
|
|
1.3.3 |
Sizes of disposable rubber gloves used in medical examination |
" |
TCVN 6343:1998 |
2 |
20 |
|
|
1.3.4 |
Sizes of sterile disposable rubber gloves used in surgery |
" |
TCVN 6344:1998 |
2 |
20 |
|
|
1.3.5 |
Rubber aging at high temperature |
(20x20) cm |
ISO 188:1982 |
7 |
30 |
|
|
1.3.6 |
Tensile test of rubber |
(20x20) cm |
ISO 37:1994 |
2 |
50 |
|
|
1.4 |
Group 4: Footwear |
02 pairs |
||||
|
1.4.1 |
Adhesiveness (tension test) between shoe soles and other details |
1 piece |
BS 5131:1978 SECTION 5.4 |
1 |
50/1 position |
|
|
1.4.2 |
Shore hardness |
(10x10) cm |
ISO 7619:1997 TCVN 1595:1988 |
1 1 |
20 20 |
|
|
1.4.3 |
Tear resistance of rubber |
(20x20) cm |
TCVN 1597:1987 |
2 |
40 |
|
|
1.4.4 |
Rubber swell degree (according to weight or volume) after being soaked in a liquid at normal temperature |
20g |
TCVN 2752:1978 |
2 |
30 |
|
|
1.4.5 |
Rubber swell degree (according to weight or volume) after being soaked in a liquid at high temperature for �days |
20g |
+30/day |
When tested at high tempera-tures |
||
|
1.4.6 |
Specific weight of rubber |
(10x10) cm |
ISO 2781:1988 |
1 |
30 |
|
|
1.4.7 |
Tensile test of rubber |
(20x20) cm |
ISO 37:1994 TCVN 4509:1988 |
2 2 |
50 50 |
|
|
1.5 |
Group 5: Latex |
1 L |
||||
|
1.5.1 |
Mechanical stability |
0.5L |
TCVN 6316:1997 ISO 35: 1995 |
2 2 |
100 100 |
|
|
1.5.2 |
Alkalinity |
0.5L |
ISO 125: 1990 TCVN 4857:1997 |
2 2 |
50 50 |
|
|
1.5.3 |
Viscosity |
0.5L |
TCVN 4859:1997 |
1 |
50 |
|
|
1.5.4 |
Rubber identification |
50g |
ASTM D 3677-90 |
2 |
170 |
|
|
Rubber identification |
50g |
ISO 4650: 1984 |
2 |
170 |
||
|
1.5.5 |
Content of dry rubber |
0.5L |
ISO 126:1995 TCVN 4858:1997 |
2 2 |
50 50 |
|
|
1.5.6 |
pH |
0.5L |
ISO 976:1996 |
1 |
30 |
|
|
1.5.7 |
Total content of solid matters |
0.5L |
ISO 124:1992 TCVN 6315:1997 |
2 2 |
50 50 |
|
|
1.5.8 |
KOH value |
0.5L |
ISO 127:1995 TCVN 4856:1997 |
2 2 |
50 50 |
|
|
1.6 |
Group 6: Bicycle inner tubes and tires |
1 piece |
||||
|
1.6.1 |
Rubber adhesiveness at inner-tube joints |
1 piece |
TCVN 1596:1988 |
1 |
20 |
|
|
1.6.2 |
Tear strength of inner-tube joints |
1 piece |
TCVN 4509:1988 |
1 |
50 |
|
|
1.6.3 |
Tensile strength of tire threads |
1 piece |
TCVN 5786:1994 |
2 |
30 |
|
|
1.6.4 |
Shore hardness |
(10x10) cm |
ISO 7619: 1997 TCVN 1595:1988 |
1 1 |
20 20 |
|
|
1.6.5 |
Aging test of rubber at high temperature |
(20x20) cm |
ISO 188: 1982 |
7 |
30/day |
|
|
1.6.6 |
Tear test of rubber |
(20x20) cm |
ISO 37: 1994 TCVN 4509: 1988 |
2 2 |
50 50 |
|
|
1.6.7 |
Abrasion test (Akron) |
(20x20) cm |
TCVN 1594: 1987 |
2 |
50 |
|
|
1.7 |
Group 7: Motorcycle inner tubes and tires |
1 piece |
||||
|
1.7.1 |
Adhesiveness of fabric layers of tires |
1 piece |
TCVN 1596:1988 |
2 |
30 |
|
|
1.7.2 |
Adhesiveness between fabric and rubber of tires |
1 piece |
TCVN 1596:1988 |
2 |
30 |
|
|
1.7.3 |
Tear strength of inner-tube joints |
1 piece |
TCVN 4509:1988 |
1 |
50 |
|
|
1.7.4 |
Tensile strength of tire threads |
1 piece |
TCVN 5786:1994 |
2 |
30 |
|
|
1.7.5 |
Shore hardness |
(10x10) cm |
ISO 7619:1997 TCVN 1595:1988 |
1 1 |
20 20 |
|
|
1.7.6 |
Tear resistance of rubber |
(20x20) cm |
TCVN 1597:1987 |
2 |
40 |
|
|
1.7.7 |
Rubber aging at high temperature |
(20x20) cm |
ISO 188: 1982 |
7 |
30/day |
|
|
1.7.8 |
Tear test of rubber |
(20x20) cm |
TCVN 4509: 1988 ISO 37: 1994 |
2 2 |
50 50 |
|
|
1.7.9 |
Abrasion test (Akron) |
(20x20) cm |
TCVN 1594: 1987 |
2 |
50 |
|
|
1.8 |
Group 8: Technical rubber products |
|||||
|
1.8.1 |
Rubber identification |
50g |
ASTM D 3677 � 90 ISO 4650: 1984 |
2 2 |
170 170 |
|
|
1.8.2 |
Tear test of rubber |
(20x20) cm |
ISO 37: 1994 TCVN 4509: 1988 |
2 2 |
50 50 |
|
|
1.8.3 |
Abrasion test (Akron) |
(20x20) cm |
TCVN 1594:1987 |
2 |
50 |
|
|
1.8.4 |
Deformation under compression |
(20x20) cm |
ISO 815: 1991 |
4 |
30 |
|
|
1.8.5 |
Specific weight |
(10x10) cm |
ISO 2781: 1988 |
1 |
30 |
|
|
1.8.6 |
Aging test of rubber at high temperature |
(20x20) cm |
ISO 188: 1982 |
7 |
30/day |
|
|
1.8.7 |
Shore hardness |
(10x10) cm |
TCVN 1595:1988 ISO 7619: 1997 |
1 1 |
20 20 |
|
|
1.8.8 |
Tear resistance of rubber |
(20x20) cm |
TCVN 1597:1987 |
2 |
40 |
|
|
1.8.9 |
Rubber swell degree (according to weight or volume) after being soaked in a liquid |
20g |
TCVN 2752:1978 |
2 |
30 |
When tested at high tempera-ture: |
|
2 |
Children�s toys |
|||||
|
2.1 |
Group 9: Children�s toys |
1 piece |
||||
|
2.1 |
Stability |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.2 |
Durability (under falling weight) |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.3 |
Dynamic durability |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.4 |
Fall durability |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.5 |
Static durability |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.6 |
Checking of hinges |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.7 |
Checking of packages |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.8 |
Checking of detachable parts |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.9 |
Checking of non-detachable parts |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.10 |
Checking of sharp points |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.11 |
Checking of fitting details |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.12 |
Checking of transmission structures |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.13 |
Checking of folding structures |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.14 |
Checking of brake structures |
1 piece |
TCVN 6238-1: 1997 |
2 |
70 |
|
|
2.15 |
Checking of immovable toys |
1 piece |
TCVN 6238-1: 1997 |
2 |
70 |
|
|
2.16 |
Checking of static-energy toys |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.17 |
Checking of toys which children can creep in |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.18 |
Checking of rocking chairs |
1 piece |
TCVN 6238-1: 1997 |
2 |
80 |
|
|
2.19 |
Checking of strings |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.20 |
Test of the distance between the body and wheel of vehicles |
1 piece |
TCVN 6238-1: 1997 |
2 |
10 |
|
|
2.21 |
Checking of springs |
1 piece |
TCVN 6238-1: 1997 |
2 |
10 |
|
|
2.22 |
Checking of sharp edges |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.23 |
Checking of overlapping joints |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.24 |
Checking of trademarks and use instructions |
1 piece |
TCVN 6238-1: 1997 |
2 |
10 |
|
|
2.25 |
Checking of tubes and hard parts |
1 piece |
TCVN 6238-1: 1997 |
2 |
40 |
|
|
2.26 |
Checking of temperature increase (after toys operate continuously for one hour) |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.27 |
Checking of stuffing materials |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.28 |
Checking of materials |
1 piece |
TCVN 6238-1: 1997 |
2 |
20 |
|
|
2.29 |
Rattles and feeding bottles |
1 piece |
TCVN 6238-1: 1997 |
2 |
50 |
|
|
2.30 |
Test of tensile strength of seam |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
2.31 |
Test by pulling off protective parts |
1 piece |
TCVN 6238-1: 1997 |
2 |
30 |
|
|
3 |
Paper |
|||||
|
3.1 |
Group 10: Corrugated paperboard |
1 m2 /1 box |
||||
|
3.1.1 |
Cracking of corrugated paperboard |
0.5 m2 |
TAPPI T 810 OM-98 |
2 |
60 |
|
|
3.1.2 |
Compression strength of corrugating edge of corrugated paperboard |
0.4 m2 |
TAPPI T 811 OM-95 |
2 |
60 |
|
|
3.1.3 |
Hardness of corrugating waves of corrugated paperboard |
0.5 m2 |
TAPPI T 808 OM-97 |
2 |
50 |
|
|
3.1.4 |
Hardness of corrugating waves of corrugated paperboard |
0.5 m2 |
TCVN 4439:1987 |
2 |
50 |
|
|
3.1.5 |
Paper fiber identification |
20g |
ISO 9184-4: 1990 |
3 |
60 |
|
|
3.1.6 |
Qualitative determination of stuffing and coating materials of paper |
20g |
ASTM D 686-93 |
3 |
60 |
|
|
3.1.7 |
pH of water solution extracted from paper |
20g |
ASTM D 778-93 |
2 |
50 |
|
|
3.2 |
Group 11: Common paper and paperboard |
1 m2 |
||||
|
3.2.1 |
Moisture |
25g |
ASTM D 644-94 ISO 287:1978 TCVN 867:1976 |
2 2 2 |
40 40 40 |
|
|
3.2.2 |
Paperboard teat strength |
0.5 m2 |
TAPPI T 807 OM-99 TCVN 3228-2:2000 |
2 2 |
60 60 |
|
|
3.2.3 |
Durability of paper |
0.5 m2 |
TCVN 1866:2000 |
2 |
50 |
|
|
3.2.4 |
Thickness of paper |
0.5 m2 |
TCVN 3652:2000 ISO 534: 1988 ASTM D 645-92 |
1 1 1 |
20 20 20 |
|
|
3.2.5 |
Crease resistance (according to circular arc) of paperboard |
0.5 m2 |
TAPPI T 822 OM-93 |
2 |
50 |
|
|
3.2.6 |
Tensile resistance of paper |
1 m2 |
ASTM D 689-92 ISO 1974:1990 TCVN 3229:2000 |
2 2 2 |
40 40 40 |
|
|
3.2.7 |
Glossiness of paper |
0.5 m2 |
ISO 8791-2:1990 |
2 |
30 |
|
|
3.2.8 |
Water absorbability of paper |
0.5 m2 |
ASTM D 3285-93 ISO 535:1991 |
2 2 |
40 40 |
|
|
3.2.9 |
Air permeability of paper |
0.5 m2 |
ISO 5636-3:1992 |
2 |
30 |
|
|
3.2.10 |
Paper fiber identification |
20g |
ISO 9184-4:1990 |
3 |
60 |
|
|
3.2.11 |
Qualitative determination n of stuffing and coating components of paper |
20g |
ASTM D 686-93 |
3 |
60 |
|
|
3.2.12 |
Ash content |
10g |
ISO 2144:1987 |
2 |
100 |
|
|
ASTM D 586-92 |
2 |
100 |
||||
|
TCVN 1864:1976 |
2 |
100 |
||||
|
3.2.13 |
Weight per square meter of paper |
0.5 m2 |
ISO 536:1995 |
2 |
30 |
|
|
3.2.14 |
pH of water solution extracted from paper |
20g |
ASTM D 778-93 |
2 |
40 |
|
|
3.2.15 |
Tensile test of paper in wet conditions |
0.5 m2 |
ASTM D 829-93 |
3 |
70 |
|
|
3.2.16 |
Tension test of paper |
0.5 m2 |
ASTM D 828-93 |
2 |
50 |
|
|
3.3 |
Group 12: Toilet tissues and paper napkins |
4-6 rolls |
||||
|
3.3.1 |
Paper moisture |
25g |
ISO 287:1987 |
2 |
40 |
|
|
3.3.2 |
Paper fiber identification |
20g |
ISO 9184-4:1990 |
3 |
60 |
|
|
3.3.3 |
Qualitative determination of stuffing and coating components of paper |
20g |
ASTM D 686-93 |
3 |
60 |
|
|
3.3.4 |
Ash content of paper |
10g |
TCVN 1864:1976 |
2 |
100 |
|
|
3.3.5 |
Weight per square meter of toilet paper |
2 rolls |
ASTM D 3905-93 |
2 |
40 |
|
|
3.3.6 |
pH of water solution extracted from paper |
20g |
ASTM D 778-93 |
2 |
50 |
|
|
3.3.7 |
Tensile test of paper in wet conditions |
0.5 m2 |
ASTM D 829-93 |
3 |
70 |
|
|
3.3.8 |
Tensile test of paper |
0.5 m2 |
ASTM D 829-93 |
2 |
50 |
|
|
3.3.9 |
Water-absorbing speed of paper |
0.5 m2 |
ASTM D 824-94 |
2 |
50 |
|
|
4 |
Plastic and plastic products |
|||||
|
4.1 |
Group 13: Plastic granules, powder, resin and polymer solution |
500 mL |
||||
|
4.1.1 |
Identification |
10g |
ASTM E 1252-94 |
2 |
170 |
|
|
4.1.2 |
Thermal stability of PVC plastic |
100g |
ASTM D 4202-92 |
2 |
50 |
|
|
4.1.3 |
Brookfield viscosity of suspension polymer in plasticization |
500 mL |
ASTM D 1824-90 |
1 |
50 |
|
|
4.1.4 |
Content of volatile substances of PVC resin |
50g |
ASTM D 3030-84 |
2 |
60 |
|
|
4.1.5 |
Ash content of thermoplastic resin |
10g |
ASTM D 5630 |
2 |
70 |
|
|
4.1.6 |
Ash content |
10g |
ISO 3451-1:1997 |
2 |
70 |
|
|
4.1.7 |
Specific weight of plastic (in powder) |
100g |
ASTM D 1895-89 |
1 |
40 |
|
|
4.1.8 |
Specific weight of plastic (in crude granules) |
100g |
ASTM D 1895-89 |
1 |
40 |
|
|
4.1.9 |
IR analysis of composition of PVC granules |
50g |
ASTM D 2124-70 |
3 |
350 |
|
|
4.2 |
Group 14: Plastic films and sheets (< 1mm) |
(50 x 50) cm |
||||
|
4.2.1 |
Changes after being soaked in liquid chemicals |
(200 x 200) mm |
ISO 175:1999 |
3 |
60 |
/1 liquid |
|
4.2.2 |
Identification |
10g |
ASTM E 1252-94 |
2 |
170 |
|
|
4.2.3 |
Adhesiveness of printing ink |
0.5 m2 |
TCVN 5820:1994 |
1 |
40 |
|
|
4.2.4 |
Adhesiveness between layers of multi-layer films |
0.5 m2 |
TCVN 5820:1994 |
1 |
40 |
|
|
4.2.5 |
Strength against chemicals |
(20 x 20)cm |
ASTM D 543-87 |
10 |
60 |
/1 chemical |
|
4.2.6 |
Strength of embossed patterns |
0.5 m2 |
TCVN 5820:1994 |
2 |
60 |
|
|
4.2.7 |
Tensile strength and breaking elongation |
0.5 m2 |
TCVN 5820:1994 |
1 |
120 |
|
|
4.2.8 |
Compression strength |
(20 x 20) cm |
ASTM D 689-92 |
2 |
100 |
|
|
4.2.9 |
Tear strength (180o anti-clockwise tear method) |
0.5 m2 |
ASTM D 1938-94 |
1 |
40 |
|
|
4.2.10 |
Tear strength |
0.5 m2 |
TCVN 5820:1994 |
1 |
40 |
|
|
4.2.11 |
Elongation after thermal aging |
0.5 m2 |
TCVN 5820:1984 |
2 |
80 |
|
|
4.2.12 |
Average mass thickness |
0.5 m2 |
TCVN 5820:1994 |
1 |
50 |
|
|
4.2.13 |
Color stainability |
0.5 m2 |
TCVN 5820:1994 |
1 |
40 |
|
|
4.2.14 |
Average thickness (PE films, sheets) |
0.5 m2 |
ASTM D 2103-92 |
1 |
50 |
|
|
4.2.15 |
Average mass thickness |
0.5 m2 |
ISO 4591:1992 |
1 |
50 |
|
|
4.2.16 |
Size stability |
0.5 m2 |
TCVN 5820:1994 |
1 |
60 |
|
|
4.2.17 |
Degree of size change under thermal effects |
0.5 m2 |
ASTM D 1204-94 |
2 |
80 |
|
|
4.2.18 |
Ash content of thermoplastic resin |
10g |
ASTM D 5630-94 |
2 |
70 |
|
|
4.2.19 |
Ash content |
10g |
ISO 3451-1:1997 |
2 |
70 |
|
|
4.2.20 |
Specific weight |
0.5 m2 |
ASTM D 729-91 |
1 |
40 |
|
|
4.2.21 |
Tendency of self-conglomeration |
0.5 m2 |
TCVN 5820:1994 |
2 |
80 |
|
|
4.2.22 |
Resilience module (tensile test) |
0.5 m2 |
ASTM D 882-91 |
1 |
120 |
|
|
4.2.23 |
Melting temperature |
1.0 dm2 |
ISO 3146:2000 |
2 |
50 |
|
|
4.2.24 |
Aging by hot air |
0.5 m |
ASTM D 1870-91 |
30 |
1/ hour |
|
|
4.3 |
Group 15: Plastic pipes and tubes (PE, PVC�), connecting accessories |
1-4 m |
||||
|
4.3.1 |
Blasting pressure |
1 m |
ASTM D 1599-88 |
1 |
100 |
|
|
4.3.2 |
Thickness of pipe or tube walls |
0.5m |
AS/NZS 1462.1-1996 |
1 |
20 |
|
|
4.3.3 |
Changes after being soaked in liquid chemicals |
(200 x 200) mm |
ISO 175:1999 |
3 |
60 |
/1 liquid |
|
4.3.4 |
Strength against sulfuric acid |
0.5 m2 |
TCVN 6037:1995 |
15 |
250 |
|
|
4.3.5 |
Strength against dichloromethane |
0.5 m2 |
ISO 7676:1990 |
1 |
70 |
|
|
4.3.6 |
Charpy impact strength |
(20 x 20) cm |
ISO 179:1993 |
1 |
60 |
|
|
4.3.7 |
Impact strength of pipes and tubes |
2 m |
AS 1462.3-1988 |
2 |
200 |
|
|
4.3.8 |
Shore D hardness |
(10x10) cm |
ISO 868:1978 |
1 |
20 |
|
|
4.3.9 |
Water absorbability (soaked for |
0.5 m2 |
ASTM D 570-81 |
2 |
80 |
24 hours) |
|
4.3.10 |
Water absorbability of PVC pipes and tubes |
0.2m |
TCVN 6042:1995 |
2 |
100 |
|
|
4.3.11 |
Outer diameter |
0.5 m2 |
TCVN 6145:1996 |
1 |
30 |
|
|
4.3.12 |
Cadmium content in extracted water |
2m |
ISO 6992:1986 |
10 |
80 |
/time |
|
4.3.13 |
Lead content in extracted water |
2m |
ISO 3114:1977 |
10 |
80 |
/time |
|
4.3.14 |
Content extracted from PVC of methanol |
100g |
ASTM D 2222-94 |
2 |
100 |
|
|
4.3.15 |
Tin content in extracted water |
2m |
ISO 3114:1977 |
10 |
80 |
/time |
|
4.3.16 |
Mercury content in extracted water |
2m |
ISO 6992:1986 |
10 |
80 |
/time |
|
4.3.17 |
Resistance against lateral compression |
0.5m |
AS 1462.2-1984 |
1 |
90 |
|
|
4.3.18 |
Resistance against high temperature |
0.5m |
AS/NZS |
2 |
200 |
|
|
4.3.19 |
Specific weight |
0.5 m2 |
ASTM D 792-91 |
1 |
40 |
|
|
4.3.20 |
Elasticity module (tensile test) |
(30 x 30) cm |
ASTM D 638-94 |
2 |
120 |
|
|
4.3.21 |
Lengthwise size changes |
1m |
TCVN 6148:1996 |
1 |
50 |
|
|
4.3.22 |
Aging with hot air |
0.5m |
ASTM D 1870-91 |
30 |
1/hour |
|
|
4.3.23 |
Tensile test of plastic (assorted pipes and tubes) |
0.5m |
ISO 6259-1:1997 |
1 |
100 |
|
|
4.3.24 |
Tensile test of plastic |
(30x30) cm |
ASTM D 638-94 |
3 |
100 |
|
|
4.4 |
Group 16: PVC tubes and pipes |
1-4m |
with cellulose core |
|||
|
4.4.1 |
Strength against chemicals |
0.5m |
KS M 3413-1992 |
1 |
60 |
/1 liquid |
|
4.4.2 |
Impact strength of pipes and tubes |
3m |
KS M 3413-1995 |
2 |
100 |
|
|
4.4.3 |
Capability against 10kV electric |
0.5m |
KS M 3413-1995 |
2 |
50 |
voltage within 1 minute |
|
4.4.4 |
Compressing force to flatten tubes |
0.5m |
KS M 3413-1995 |
1 |
100 |
and pipes |
|
4.4.5 |
Thermal strength test |
0.5m |
KS M 3413-1995 |
1 |
50 |
|
|
4.5 |
Group 17: Plastic sheets |
(50 x 50) cm |
||||
|
4.5.1 |
Changes after being soaked in liquid chemicals |
(200 x 200) mm |
ISO 175:1999 |
3 |
60 |
/1 liquid |
|
4.5.2 |
Identification |
10g |
ASTM E 1252-94 |
2 |
170 |
|
|
4.5.3 |
Moisture (of ceiling sheets composed of cellulose fiber) |
(20 x 25) cm |
ASTM C 209-92 |
1 |
40 |
|
|
4.5.4 |
Strength against chemicals |
(20 x 20) cm |
ASTM D 543-87 |
10 |
60 |
/1 liquid |
|
4.5.5 |
Tensile strength (of ceiling sheets composed of cellulose fiber) |
(20 x 25) cm |
ASTM C 209-92 |
1 |
60 |
|
|
4.5.6 |
Compression strength |
(20 x 20) cm |
ISO 604:1993 |
2 |
100 |
|
|
4.5.7 |
Flexing strength |
1 ml |
ISO 178:1993 |
1 |
100 |
|
|
4.5.8 |
Charpy impact strength |
(20x20) cm |
ISO 179:1993 |
1 |
60 |
|
|
4.5.9 |
Shore D hardness |
(10x10) cm |
ISO 868:1978 |
1 |
20 |
|
|
4.5.10 |
Water absorbability (after being soaked for 24 hours) |
0.5 m2 |
ASTM D 570-81 |
2 |
80 |
|
|
4.5.11 |
Size changes under thermal effects |
0.5 m2 |
ASTM D 1204-94 |
2 |
80 |
|
|
4.5.12 |
Lost contents due to baking |
50g |
ASTM D 2584-94 |
2 |
80 |
|
|
4.5.13 |
Content of glass fiber |
50g |
JIS K 7052:1987 |
2 |
80 |
|
|
4.5.14 |
Ash content of thermoplastic resin |
10g |
ASTM D 5630-94 |
2 |
70 |
|
|
4.5.15 |
Specific weight |
0.5 m2 |
ASTM D 792-91 |
1 |
40 |
|
|
4.5.16 |
Specific weight (of ceiling sheets composed of cellulose fiber) |
(10x10) cm |
ASTM C 209-92 |
1 |
60 |
|
|
4.5.17 |
Resilience module (tensile test) |
(30x30) cm |
ASTM D 638-94 |
2 |
120 |
|
|
4.5.18 |
Aging with hot air |
0.5m |
ASTM D 1870-91 |
30 |
1/hour |
|
|
4.5.19 |
Tensile test of plastic |
(30x30) cm |
ISO 527-1:1993 |
1 |
100 |
|
|
4.5.20 |
Burning speed of plastic sheets along lateral direction |
(20 x 20) cm |
ASTM D 635-91 |
1 |
80 |
|
|
4.6 |
Group 18: Plastic coverings |
2 m2 |
2 |
170 |
||
|
4.6.1 |
Identification |
10g |
ASTM E 1252-94 |
2 |
170 |
|
|
4.6.2 |
Rubber identification |
50g |
ASTM D 3677-90 |
2 |
170 |
|
|
4.6.3 |
Adhesiveness of covering layer |
500 cm2 |
TCVN 4638:1988 |
2 |
100 |
|
|
4.6.4 |
Tensile strength and breaking elongation |
500 cm2 |
ISO 1421:1998 |
1 |
60 |
|
|
4.6.5 |
Color fastness in artificial light (Xenon lighting source) |
100 cm2 |
ISO 105-B 02:1994 |
30 |
500 |
|
|
4.6.6 |
Color fastness in artificial light (high-pressure mercury lamps) |
0.2 m2 |
TCVN 5823:1994 |
15 |
100 |
|
|
4.6.7 |
Explosion strength |
(30 x 30) cm |
TCVN 5826:1994 |
1 |
60 |
|
|
4.6.8 |
Folding strength |
0.1 m2 |
TCVN 5821:1994 |
30 |
200 |
1/day |
|
4.6.9 |
Thickness |
200 cm2 |
ISO 2286-3:1998 |
1 |
20 |
|
|
4.6.11 |
Anti-conglomeration capability |
0.2 m2 |
ISO 5978:1990 |
3 |
80 |
|
|
4.6.12 |
Weight of covering film/acreage unit |
600 cm2 |
TCVN 5827:1994 |
2 |
100 |
|
|
4.6.13 |
Aggregate weight/acreage unit |
600 cm2 |
TCVN 5827:1994 |
1 |
50 |
|
|
4.6.14 |
Tear force |
500 cm2 |
ISO 4674:1977 |
1 |
60 |
|
|
4.7 |
Group 19: Hard cellulose materials |
3 sheets/ (50x50) cm |
||||
|
4.7.1 |
Identification |
10g |
ASTM E 1252-94 |
2 |
170 |
|
|
4.7.2 |
Tensile strength and breaking elongation |
(30x30) cm |
ISO 1926:1979 |
1 |
100 |
|
|
4.7.3 |
Compression strength |
(20x20) cm |
ASTM D 1621-94 |
1 |
100 |
|
|
4.7.4 |
Water absorbability (soaked for 24 hours) |
0.5 m2 |
ASTM D 1570-81 |
2 |
80 |
|
|
4.7.5 |
Water absorbability (soaked for 96 hours) |
1,500 cm3 |
ISO 2896:1987 |
5 |
120 |
|
|
4.7.6 |
Specific weight |
(10x10) cm |
ASTM D 1622-93 |
1 |
40 |
|
|
4.7.7 |
Aging with hot air |
0.5m |
ISO 2440:1997 |
30 |
1/hour |
|
|
4.7.8 |
Test by burning cellulose material along horizontal direction |
1500 cm3 |
ISO 3582:1978 |
3 |
130 |
|
|
4.8 |
Group 20: Soft cellulose materials |
3 sheets/ (50x50) cm |
||||
|
4.8.1 |
Deformations under excessive compression |
(30x30) cm |
ISO 1856:1980 |
3 |
80 |
|
|
4.8.2 |
Hardness index (sinking test) |
(40x40) cm |
ISO 2439:1997 |
1 |
100 |
|
|
4.8.3 |
Hardness characteristics (sinking test) |
(40x40) cm |
ISO 2439:1997 |
1 |
100 |
|
|
4.8.4 |
Identification |
10g |
ASTM E 1252-94 |
2 |
170 |
|
|
4.8.5 |
Tensile strength and breaking elongation |
(30x30) cm |
ISO 1798:1997 |
1 |
100 |
|
|
4.8.6 |
Compression strength |
(20x20) cm |
ISO 3386-1:1986 |
2 |
100 |
|
|
4.8.7 |
Specific weight |
(10x10) cm |
ISO 845:1988 |
1 |
40 |
|
|
4.8.8 |
Aging with hot air |
0.5m |
ISO 2440:1997 |
30 |
1/hour |
|
|
4.8.9 |
Test by burning cellulose material along lateral direction |
1500 cm3 |
ASO 3582:1978 |
3 |
150 |
|
|
5 |
Paints |
|||||
|
5.1 |
Group 21: Alkyd paint |
1 kg |
||||
|
5.1.1 |
Acid index |
100g |
ASTM D 1639-90 |
1 |
40 |
|
|
5.1.2 |
Evaluation of paint film under the conditions of artificial weather |
200g |
JIS K 5400:1990 |
7-30 |
300 |
300/day |
|
5.1.3 |
Identification of resin separated from paint |
100g |
ASTM D 2621-87 |
3 |
300 |
|
|
5.1.4 |
Adhesiveness of film |
100g |
TCVN 2097:1993 |
2 |
30 |
|
|
5.1.5 |
Optical brightness (the ray�s angle is up to 60o) |
100g |
TCVN 2101:1993 |
2 |
30 |
|
|
5.1.6 |
Film �s strength against acids |
100g |
JSK K 5400:1990 |
2 |
50 |
|
|
5.1.7 |
Film�s strength against household chemicals |
100g |
ASTM D 1308-87 |
30 |
40 |
|
|
5.1.8 |
Film�s strength against alkali |
100g |
JIS K 5400:1990 |
2 |
40 |
/1 chemical |
|
5.1.9 |
Film�s strength against saline water |
100g |
JIS K 5400: 1990 |
5 |
50 |
|
|
5.1.10 |
Film�s strength against boiling water |
100g |
JIS K 5400: 1990 |
1 |
50 |
|
|
5.1.11 |
Color fastness in artificial light |
200g |
ISO 2809:1976 |
7-9 |
500 |
|
|
5.1.12 |
Film�s flexing strength |
100g |
TCVN 2099:1993 |
2 |
30 |
|
|
5.1.13 |
Film�s impact strength |
100g |
ASTM D 2794-93 |
2 |
30 |
|
|
5.1.14 |
Paint film�s impact strength |
100g |
TCVN 2100:1993 |
2 |
30 |
|
|
5.1.15 |
Film�s hardness against scratch |
100g |
ISO 10005:1995 |
2 |
30 |
|
|
5.1.16 |
Hardness of film pendulum |
100g |
ASTM D 4366-94 |
2 |
30 |
|
|
5.1.17 |
Fineness of paint |
100g |
ISO 1524:1983 JIS K 5400: 1990 ASTM D 1210-79 TCVN 2091:1993 |
1 1 1 1 |
20 20 20 20 |
|
|
5.1.18 |
The Brookfield viscosity (at 25o C) of paint, solvent and similar substances |
500 mL |
ASTM D 2196-86 |
1 |
50 |
|
|
5.1.19 |
Conventional viscosity of paint |
500 mL |
TCVN 2092:1993 |
1 |
30 |
|
|
5.1.20 |
Coverage |
500g |
TCVN 2095:1993 |
2 |
40 |
|
|
5.1.21 |
Content of color powders in paint |
200g |
ASTM D 2371-85 |
3 |
60 |
|
|
5.1.22 |
Content of non-volatile substances (calculated by volume) |
100g |
ASTM D 2697-86 |
7 |
200 |
|
|
5.1.23 |
Content of non-volatile substances |
100g |
ISO 1515:1973 JIS K 5407: 1990 ASTM D 2369-93 |
1 1 1 |
40 40 40 |
|
|
5.1.24 |
Content of resin in paint |
100g |
ASTM D 2372-85 |
1 |
60 |
|
|
5.1.25 |
Thermal resistance of film |
100g |
JIS K 5400:1990 |
3 |
120 |
|
|
5.1.26 |
Thermal resistance of film (within 24 hours) |
100g |
ASTM D 2485-91 |
2 |
100 |
|
|
5.1.27 |
Specific weight of paint |
400mL |
JIS K 5400:1990 |
1 |
40 |
|
|
5.1.28 |
Specific weight of paint, varnishes |
100mL |
ASTM D 1475-90 |
1 |
40 |
|
|
5.1.29 |
Drying time of paint |
100g |
ASTM D 1640-83 |
2 |
20 |
|
|
5.2 |
Group 22: Rubber paint |
1kg |
||||
|
5.2.1 |
Rubber identification |
50g |
ASTM D 3677-90 |
2 |
300 |
|
|
5.2.2 |
Identification of resin separated from paint |
100g |
ASTM D 2621-87 |
3 |
300 |
|
|
5.2.3 |
Optical brightness (the ray�s angle is up to 60o) |
100g |
TCVN 2101:1992 |
2 |
30 |
|
|
5.2.4 |
Film�s strength against alkali |
100g |
JIS K 5639:1989 |
2 |
40 |
|
|
5.2.5 |
Film�s strength against saline water |
100g |
JIS K 5639:1989 |
8 |
50 |
|
|
5.2.6 |
Color fastness in artificial light (Xenon lighting source) |
200g |
ISO 2809:1976 |
7-9 |
500 |
|
|
5.2.7 |
Film�s flexing strength |
100g |
JIS K 5639:1989 |
2 |
30 |
|
|
5.2.8 |
Fineness of paint |
100g |
ASTM D 1210-79 |
1 |
20 |
|
|
5.2.9 |
Content of non-volatile substances (calculated by volume) |
100g |
ASTM D 2697-86 |
7 |
200 |
|
|
5.2.10 |
Specific weight of paint |
400mL |
JIS K 5400:1990 |
1 |
40 |
|
|
5.2.11 |
Specific weight of paint and varnishes |
400mL |
|
|
|
|
|
5.2.12 |
Drying time of paint |
100g |
ASTM D 1640-83 |
2 |
20 |
|
|
5.2.13 |
Test of double coverings |
200g |
JIS K 5639:1989 |
2 |
50 |
|
|
5.3 |
Group 23: Solvent paints |
1kg |
||||
|
5.3.1 |
Acid value |
100g |
ASTM D 1639-90 |
1 |
40 |
|
|
5.3.2 |
Evaluation of the paint�s film under the impact of artificial weather |
200g |
JIS K 5400:1990 |
7-30 |
300 |
300/day |
|
5.3.3 |
Rubber identification |
50g |
ISO 4650:1984 |
2 |
170 |
|
|
5.3.4 |
Identification of resin separated from rubber |
100g |
ASTMD D 2612-87 |
3 |
300 |
|
|
5.3.5 |
Adhesiveness of film |
100g |
TCVN 2097:1993 |
2 |
30 |
|
|
5.3.6 |
Film�s adhesiveness against acids |
100g |
JIS K 5400:1990 |
2 |
50 |
|
|
5.3.7 |
Film�s adhesiveness against household chemicals |
100g |
ASTM D 1308-87 |
30 |
40 |
|
|
5.3.8 |
Film�s strength against alkali |
100g |
JIS K 5400:1990 |
2 |
40 |
|
|
5.3.9 |
Film�s strength against saline water |
100g |
JIS K 5400:1990 |
5 |
50 |
|
|
5.3.10 |
Film�s strength against boiling water |
100g |
JIS K 5400:1990 |
1 |
50 |
|
|
5.3.11 |
Ink film�s strength against water |
100g |
ASTM D 1647-89 |
2 |
40 |
|
|
5.3.12 |
Color fastness in artificial light (Xenon lighting source) |
200g |
ISO 2809:1976 |
7-9 |
500 |
|
|
5.1.13 |
Film�s flexing strength |
100g |
TCVN 2099:1993 |
2 |
30 |
|
|
5.3.14 |
Paint film�s impact strength |
100g |
TCVN 2100:1993 |
2 |
30 |
|
|
5.3.15 |
Optical brightness (the ray�s angle is up to 60o) |
100g |
JIS K 5400:1990 |
2 |
30 |
|
|
5.3.16 |
Film�s hardness against scratch |
100g |
ISO 10005:1995 |
2 |
30 |
|
|
5.3.17 |
Film�s pendulum hardness |
100g |
TCVN 2098:1993 |
2 |
30 |
|
|
5.3.18 |
Fineness of paint |
100g |
TCVN 2082:1977 JIS K 5400:1990 ASTM D 1210-79 ISO 1524:1983 TCVN 2091:1993 |
1 1 1 1 1 |
20 20 20 20 20 |
|
|
5.3.19 |
The Brookfield viscosity (at 25o C) of paint, solvent and similar substances |
500mL |
ASTM D 2196-86 |
1 |
50 |
|
|
5.3.20 |
Conventional viscosity of strong printing ink |
500mL |
TCVN 2084:1997 |
1 |
30 |
|
|
5.3.21 |
Conventional viscosity of weak printing ink |
500mL |
TCVN 2083:1977 |
1 |
30 |
|
|
5.3.22 |
Conventional viscosity of paint |
500mL |
TCVN 2092:1993 |
1 |
30 |
|
|
5.3.23 |
Coverage |
500g |
TCVN 2095:1993 |
2 |
40 |
|
|
5.3.24 |
Water absorbability of dry film |
100g |
JIS K 5400:1990 |
2 |
50 |
|
|
5.3.25 |
Content of color powder in paint |
200g |
ASTM D 2371-85 |
3 |
60 |
|
|
5.3.26 |
Content of non-volatile substances (calculated by volume) |
100g |
ASTM D 2697-86 |
7 |
200 |
|
|
5.3.27 |
Content of non-volatile substances of paint or varnish solutions |
50g |
ASTM D 4209 |
1 |
40 |
|
|
5.3.28 |
Content of non-volatile substances of ink |
100g |
ASTM D 2241-93 |
1 |
40 |
|
|
5.3.29 |
Content of non-volatile substances of paint |
100g |
JIS K 5407:1990 |
1 |
40 |
|
|
5.3.30 |
Content of non-volatile substances of road paint |
100g |
ASTM D 1644-88 |
1 |
40 |
|
|
5.3.31 |
Content of resin in paint |
100g |
ASTM D 2372-85 |
1 |
60 |
|
|
5.3.32 |
Film�s heat resistance |
100g |
JIS K 5400:1990 ASTM D 2485-91 |
3 3 |
120 300 |
|
|
5.3.33 |
Film�s heat resistance (within 24 hours) |
100g |
ASTM D 1485-91 |
2 |
100 |
|
|
5.3.34 |
Specific weight of paint |
400mL |
JIS K 5400:1990 |
1 |
40 |
|
|
5.3.35 |
Specific weight of paint or varnishes |
400mL |
ISO 2811-1:1997 |
1 |
40 |
|
|
5.3.36 |
Drying time of paint |
100g |
JIS K 5400:1990 ASTM D 1640-83 TCVN 2096:1993 |
2 2 2 |
20 20 20 |
|
|
5.3.37 |
Drying time of ink |
100g |
TCVN 2087:1977 |
1 |
20 |
|
|
5.3.38 |
Total content of poisonous elements (Cu+) of anti-fouling paint |
100g |
JIS K 5101 (1964) |
8 |
150 |
|
|
5.4 |
Group 24: Epoxy paint |
1kg |
||||
|
5.4.1 |
Identification of resin separated from paint |
100g |
ASTM D 2621-87 |
3 |
300 |
|
|
5.4.2 |
Adhesiveness of film |
100g |
ASTM D 3359-93 TCVN 2097:1993 JIS K 5400:1990 |
2 2 2 |
30 30 30 |
|
|
5.4.3 |
Film�s strength against alkali |
100g |
JIS K 5551:1991 |
7 |
40 |
|
|
5.4.4 |
Film�s strength against saline water |
100g |
JIS K 5551:1991 |
10 |
50 |
|
|
5.4.5 |
Film�s strength against petrol |
100g |
JIS K 5551:1991 |
2 |
40 |
|
|
5.4.6 |
Film�s strength against water (after 500 hours at 66oC) |
100g |
AWW A C 550-90 |
22 |
600 |
30/day |
|
5.4.7 |
Color fastness in artificial light (Xenon lighting source) |
200g |
ISO 2809:1976 |
7-9 |
500 |
|
|
5.4.8 |
Paint film�s impact strength |
100g |
TCVN 2100:1993 ASTM D 2794-93 |
2 2 |
30 30 |
|
|
5.4.9 |
Optical brightness (the ray�s angle is up to 60o) |
100g |
TCVN 2101:1993 JIS K 5400:1990 ASTM D 523-89 |
2 2 2 |
30 30 30 |
|
|
5.4.10 |
Fineness of paint |
100g |
TCVN 2091:1993 ISO 1524:1983 JIS K 5400:1990 ASTM D 1210-79 |
1 1 1 1 |
20 20 20 20 |
|
|
5.4.11 |
Content of non-volatile substances (calculated by volume) |
100g |
ASTM D 2697-86 |
7 |
200 |
|
|
5.4.12 |
Content of non-volatile substances of paint |
100g |
JIS K 5407:1990 ISO 1515:1973 ASTM D 2369-93 |
1 1 1 |
40 40 40 |
|
|
5.4.13 |
Specific weight of paint |
400mL |
JIS K 5400:1990 |
1 |
40 |
|
|
5.4.14 |
Specific weight of paint or varnish |
100mL 400mL |
ASTM D 1475-90 ISO 2811-1:1997 |
1 1 |
40 40 |
|
|
5.4.15 |
Drying time of paint |
100g |
JIS K 5400:1990 ASTM D 1640-83 |
2 2 |
20 20 |
|
|
5.5 |
Group 25: Nitrocellulose paints |
1kg |
||||
|
5.5.1 |
Identification of resin separated |
100g |
ASTM D 2621-87 |
3 |
300 |
from paint |
|
5.5.2 |
Adhesiveness of film |
100g |
ASTM D 3359-93 |
2 |
30 |
|
|
TCVN 2097:1993 JIS K 5400:1990 |
2 2 |
30 30 |
||||
|
5.5.3 |
Film�s strength against water |
100g |
JIS K 5531:1992 |
1 |
40 |
|
|
5.5.4 |
Film�s strength against boiling water |
100g |
JIS K 5531:1992 |
1 |
50 |
|
|
5.5.5 |
Film�s strength against petrol |
100g |
JIS K 5531:1992 |
2 |
40 |
|
|
5.5.6 |
Conglomeration strength |
100g |
JIS K 5531:1992 |
1 |
50 |
|
|
5.5.7 |
Color fastness in artificial light (Xenon lighting source) |
200g |
ISO 2809:1976 |
7-9 |
500 |
|
|
5.5.8 |
Optical brightness (the ray�s angle is up to 60o) |
100g |
TCVN 2101:1993 JIS K 5400:1990 ASTM D 523-89 |
2 2 2 |
30 30 30 |
|
|
5.5.9 |
Fineness of paint |
100g |
ASTM D 1210-79 ISO 1524:1983 JIS K 5400:1990 TCVN 2091:1993 |
1 1 1 1 |
20 20 20 20 |
|
|
5.5.10 |
Content of non-volatile substances (calculated by volume) |
100g |
ASTM D 2697-86 |
7 |
200 |
|
|
5.5.11 |
Content of non-volatile substances of resin or varnish solutions |
50g |
ASTM D 4209 |
1 |
40 |
|
|
5.5.12 |
Content of non-volatile substances of paint |
100g |
ASTM D 2369-93 ISO 1515:1973 JIS K 5407:1990 |
1 1 1 |
40 40 40 |
|
|
5.5.13 |
Specific weight of paint |
100g 400mL |
JIS K 5531:1992 JIS K 5400:1990 |
2 1 |
120 40 |
|
|
5.5.14 |
Specific weight of paint or varnish |
400mL 100mL |
ISO 2811-1:1997 ASTM D 1475-90 |
1 1 |
40 40 |
|
|
5.5.15 |
Drying time of paint |
100g |
JIS K 5400:1990 |
2 |
20 |
|
|
5.6 |
Group 26: PU paints |
1kg |
||||
|
5.6.1 |
Identification of resin separated from paint |
100g |
ASTM D 2621-87 |
3 |
300 |
|
|
5.6.2 |
Adhesiveness of film |
100g |
TCVN 2097:1993 ASTM D 3359-93 JIS K 5400:1990 |
2 2 2 |
30 30 30 |
|
|
5.6.3 |
Film�s strength against acids |
100g |
JIS K 5400:1990 |
2 |
50 |
|
|
5.6.4 |
Film�s strength against alkali |
100g |
JIS K 5656:1992 |
7 |
50 |
|
|
5.6.5 |
Color fastness in artificial light (Xenon lighting source) |
200g |
ISO 2809:1976 |
7-9 |
500 |
|
|
5.6.6 |
The paint film�s impact strength |
100g |
TCVN 2100:1993 |
2 |
30 |
|
|
5.6.7 |
Optical brightness (the ray�s angle is up to 60o) |
100g |
TCVN 2010:1993 JIS K 5656:1992 JIS K 5400:1990 ASTM D 523-89 |
2 1 2 2 |
30 30 30 30 |
|
|
5.6.8 |
Fineness of paint |
100g |
TCVN 2091:1993 ISO 1524:1983 JIS K 5400:1990 ASTM D 1210-79 |
1 1 1 1 |
20 20 20 20 |
|
|
5.6.9 |
Content of non-volatile substances of |
100g |
ASTM D 2369-93 ISO 1515:1973 JIS K 5407:1990 |
1 1 1 |
40 40 40 |
|
|
5.6.10 |
Content of non-volatile substances (calculated by volume) |
100g |
ASTM D 2697-86 |
7 |
200 |
|
|
5.6.11 |
Re-coverability |
100g |
JIS K 5656:1992 |
7 |
50 |
|
|
5.6.12 |
Drying time of paint |
100g |
ASTM D 1640-83 JIS K 5400:1990 |
2 2 |
20 20 |
|
|
5.7 |
Group 27: Electrostatic dipping paint |
1kg |
||||
|
5.7.1 |
Electric conductivity |
100g |
ASTM D 4399-90 |
2 |
80 |
|
|
5.7.2 |
pH |
100g |
ASTM D 4584-86 |
1 |
30 |
|
|
5.7.3 |
Acid content |
100g |
ASTM D 4218-91 |
1 |
120 |
|
|
5.7.4 |
Content of non-volatile substances |
100g |
ASTM D 5145-90 |
1 |
60 |
|
|
5.8 |
Group 28: Water paints |
1kg |
||||
|
5.8.1 |
Identification of polymer in emulsion paint |
250mL |
ASTM D 3168-85 |
2 |
300 |
|
|
5.8.2 |
Film�s strength against household chemicals |
100g |
ASTM D 1308-87 |
30 |
40 |
|
|
5.8.3 |
Film�s strength against alkali |
100g |
JIS K 5960 (1983) |
3 |
30 |
|
|
5.8.4 |
Film�s strength against water |
100g |
ASTM D 870-92 JIS K 5960 (1983) |
1 4 |
40 40 |
|
|
5.8.5 |
Film�s strength against water in frost-spraying conditions |
100g |
ASTM D 1735-92 |
7 |
350 |
|
|
5.8.6 |
Color fastness in artificial light (Xenon lighting source) |
200g |
ISO 2809:1976 |
7-9 |
500 |
|
|
5.8.7 |
Electric conductivity |
200g |
ASTM D 1000-93 |
2 |
40 |
|
|
5.8.8 |
Fineness of paint |
100g |
ISO 1524:1983 TCVN 2091:1993 ASTM D 1210-79 |
1 1 1 |
20 20 20 |
|
|
5.8.9 |
The Brookfield viscosity of paint, resin solution and similar substances |
500mL |
ASTM D 2196-86 |
1 |
50 |
|
|
5.8.10 |
pH |
100g |
ASTM E 70-90 |
1 |
50 |
|
|
5.8.11 |
Coverage |
500g |
JIS K 5960 (1983) |
2 |
40 |
|
|
5.8.12 |
Water absorbability of dry film |
100g |
JIS K 5400:1990 |
2 |
50 |
|
|
5.8.13 |
Stability at low temperature |
500g |
JIS K 5960 (1983) |
5 |
200 |
|
|
5.8.14 |
Content of color powder in paint |
200g |
ASTM D 2371-85 |
3 |
60 |
|
|
5.8.15 |
Content of color powder in emulsion paint (test by baking at low temperature) |
100g |
ASTM D 3723-84 |
1 |
100 |
|
|
5.8.16 |
Content of non-sifted substances |
100g |
ASTM D 185-84 |
1 |
60 |
|
|
5.8.17 |
Content of non-volatile substances |
100g |
ASTM D 2369-93 ISO 1515:1973 |
1 1 |
40 40 |
|
|
5.8.18 |
Specific weight |
400mL 100mL |
ISO 2811-1:1997 ASTM D 1475-90 |
1 1 |
40 40 |
|
|
5.8.19 |
Outer appearance of paint |
500g |
JIS K 5960 (1983) |
2 |
30 |
|
|
5.8.20 |
Drying time of paint |
100g |
ASTM D 1640-83 JIS K 5960 (1983) |
2 2 |
20 20 |
|
|
5.8.21 |
Test of double covering |
200g |
JIS K 5960 (1983) |
2 |
50 |
|
|
6 |
Fabric, yarn |
|||||
|
6.1 |
Group 29: Yarn |
1 set |
||||
|
6.1.1 |
Yarn index |
1,000m |
TCVN 5785:1994 |
1 |
30 |
|
|
6.1.2 |
Identification |
10g |
ASTM D 276-87 |
2 |
170 |
|
|
6.1.3 |
Moisture |
100g |
TCVN 1750:1986 |
1 |
40 |
|
|
6.1.4 |
Color fastness in artificial light (Xenon lighting source) |
100 cm2 |
ISO 105-B02:1994 |
30 |
500 |
|
|
6.1.5 |
Color fastness in artificial light (high- pressure mercury lighting source) |
0.2 m2 |
TCVN 5823:1994 |
15 |
100 |
|
|
6.1.6 |
Color fastness in solvents |
0.2 m2 |
BS EN ISO 105-X05 |
2 |
50 |
/1 solvent |
|
6.1.7 |
Color fastness in water |
0.2 m2 |
BS EN ISO 105- E01: 1996 |
2 |
40 |
|
|
6.1.8 |
Color fastness in seawater |
0.2 m2 |
TCVN 2533:1990 BS EN ISO 105 - E02:1996 |
2 2 |
50 50 |
|
|
6.1.9 |
Color fastness in chlorine |
0.2 m2 |
BS EN ISO 105- E03:1997 |
2 |
50 |
|
|
6.1.10 |
Color fastness in hot pressing (dry and wet pressing) |
0.2 m2 |
BS EN ISO 105- X11:1996 |
2 |
100 |
|
|
6.1.11 |
Color fastness in washing (detergents) |
0.2 m2 |
ISO 105-C06:1994 |
2 |
50 |
|
|
6.1.12 |
Color fastness in soap-washing |
0.2 m2 |
TCVN 4537:1988 ISO 105-C01:1989 |
2 2 |
50 50 |
|
|
6.1.13 |
Color fastness in hot dry ironing |
0.2 m2 |
TCVN 5011:1989 |
1 |
30 |
|
|
6.1.14 |
Color fastness in hot wet ironing |
0.2 m2 |
TCVN 5011:1989 |
1 |
30 |
|
|
6.1.15 |
Color fastness in sweat |
0.2 m2 |
BS EN ISO 105- E04:1996 |
2 |
100 |
|
|
6.1.16 |
Color fastness in thermal treatment |
0.2 m2 |
BS EN ISO 105- P01:1995 |
2 |
50 |
|
|
6.1.17 |
Strength and elongation when a single warp is pulled apart |
1,000m |
TCVN 5786:1994 |
1 |
50 |
|
|
6.1.18 |
Twist � Twist direction |
1,000m |
TCVN 5788:1994 |
1 |
30 |
|
|
6.1.19 |
Quantitative analysis of yarn mixture |
20g |
ASTM D 629-95 |
2 |
200 |
|
|
6.2 |
Group 30: Fabric, clothes |
1 set |
||||
|
6.2.1 |
Identification |
10g |
ASTM D 276-87 |
2 |
170 |
|
|
6.2.2 |
Moisture |
100g |
TCVN 1750:1986 |
1 |
40 |
|
|
6.2.3 |
Tensile strength of bands of knitted fabric |
0.5 m2 |
TCVN 5795:1994 |
1 |
50 |
|
|
6.2.4 |
Tensile strength of bands and elongation at the time of pulling apart woven fabric |
0.5 m2 |
TCVN 1754:1986 |
1 |
50 |
|
|
6.2.5 |
Tensile strength and elongation of non-woven fabric |
40x40 cm |
ISO 9073-3:1989 |
2 |
50 |
|
|
6.2.6 |
Color fastness in artificial light (high- pressure mercury lights) |
0.2 m2 |
TCVN 5823:1994 |
15 |
100 |
|
|
6.2.7 |
Color fastness in artificial light (Xenon lighting source) |
0.2 m2 |
ISO 105-B02:1994 |
15 |
500 |
|
|
6.2.8 |
Color fastness in sodium hypochloride solution |
0.2 m2 |
TCVN 5473:1991 |
2 |
70 |
|
|
6.2.9 |
Color fastness in solvents |
0.2 m2 |
BS EN ISO 105- X05:1997 |
2 |
50 |
/1 solvent |
|
6.2.10 |
Color fastness in seawater |
0.2 m2 |
BS EN ISO 105- E02:1996 TCVN 5233:1990 |
2 2 |
50 50 |
|
|
6.2.11 |
Color fastness in chloride liquid |
0.2 m2 |
BS EN ISO 105- E03:1997 TCVN 5234:1990 |
2 2 |
50 50 |
|
|
6.2.12 |
Color fastness in water |
0.2 m2 |
BS EN ISO 105- E01:1996 TCVN 5074:1990 |
2 2 |
40 40 |
|
|
6.2.13 |
Color fastness in hot pressing (dry and wet pressing) |
0.2 m2 |
BS EN ISO 105- X11:1996 |
2 |
100 |
|
|
6.2.14 |
Color fastness in washing (detergents) |
0.2 m2 |
ISO 105-C06:1994 |
2 |
50 |
|
|
6.2.15 |
Color fastness in soap-washing |
0.2 m2 |
ISO 105-C01:1989 |
2 |
50 |
|
|
6.2.16 |
Color fastness in hot dry ironing |
0.2 m2 |
TCVN 4537:1988 TCVN 5011:1989 TCVN 5011:1989 |
2 1 1 |
50 30 30 |
|
|
6.2.17 |
Color fastness in dry friction |
0.2 m2 |
BS EN ISO 105- X12:1995 TCVN 4538:1994 |
2 1 |
30 30 |
|
|
6.2.18 |
Color fastness in wet friction |
0.2 m2 |
BS EN ISO 105- X12:1997 TCVN 4538:1994 |
2 1 |
30 30 |
|
|
6.2.19 |
Color fastness in sweat |
0.2 m2 |
BS EN ISO 105- E04:1996 TCVN 5235:1990 |
2 2 |
100 60 |
|
|
6.2.20 |
Color fastness in dry thermal treatment |
0.2 m2 |
BS EN ISO 105- P01:1995 |
2 |
50 |
|
|
6.2.21 |
Thickness of knitted fabric |
0.5 m2 |
TCVN 5071:1990 |
1 |
30 |
|
|
6.2.22 |
Thickness of woven fabric |
0.5 m2 |
TCVN 5071:1990 |
1 |
30 |
|
|
6.2.23 |
Smallness of yarn separated from woven fabric |
0.6 m2 |
TCVN 5095:1990 |
1 |
40 |
|
|
6.2.24 |
Twist of yarn separated from woven fabric |
0.6 m2 |
TCVN 5094:1990 |
1 |
40 |
|
|
6.2.25 |
Content of free formaldehyde |
0.2 m2 |
ISO 14184-1:1998 |
2 |
100 |
|
|
6.2.26 |
Weight of woven fabric |
0.5 m2 |
TCVN 1752:1986 |
1 |
30 |
|
|
6.2.27 |
Weight per square meter of knitted fabric |
1 m2 |
TCVN 5793:1994 |
1 |
30 |
|
|
6.2.28 |
Weight per square meter of non-woven fabric |
1 m2 |
ISO 9073-1:1989 |
2 |
40 |
|
|
6.2.29 |
Sizes of knitted and woven fabric |
1 m2 |
TCVN 5792:1994 TCVN 1751:1986 |
1 1 |
20 20 |
|
|
6.2.30 |
Force of piercing geotechnical fabric |
1 m2 |
ISO 12236:1996 |
1 |
100 |
|
|
6.2.31 |
Yarn density of knitted and woven fabric |
1 m2 |
TCVN 5794:1994 TCVN 1753:1986 |
1 1 |
40 40 |
|
|
6.2.32 |
Size changes of knitted fabric after washing |
1 m2 |
TCVN 5798:1994 |
2 |
50 |
|
|
6.2.33 |
Size changes of woven fabric after washing |
1 m2 |
TCVN 1755:1986 |
2 |
50 |
|
|
6.2.34 |
Quantitative analysis of yarn mixture |
20g |
ASTM D 629-95 |
2 |
200 |
DOMAIN: CONSTRUCTION
|
Ordinal number |
Product names - criteria |
Quantity |
Testing method |
Duration day |
Unit price VND 1,000 |
Notes |
|
1 |
Cement |
10 kg |
30 |
|||
|
1.1 |
Fineness after sieving |
TCVN 4030:1985 |
20 |
|||
|
1.2 |
Crushing fineness (acclive surface) |
TCVN 4030:1985 |
30 |
|||
|
1.3 |
Concretion time |
TCVN 6017:1995 |
30 |
|||
|
1.4 |
Volume stability |
TCVN 6017:1995 |
30 |
|||
|
1.5 |
Compression intensity 3, 28 days |
BSEN 196.1-1995 |
300 |
Foreign sand |
||
|
1.6 |
Specific weight |
TCVN 4030:1985 |
30 |
|||
|
1.7 |
Standard water content |
TCVN 6017:1995 |
20 |
|||
|
1.8 |
Autoclave expansion |
ASTM C 151-98a |
200 |
|||
|
1.9 |
Sulfate expansion |
ASTM C 452-95 |
400 |
|||
|
2 |
Fibro-cement roofing sheets |
1 sheet |
TCVN 4435:1992 |
5 |
||
|
2.1 |
Basic dimensions |
20 |
||||
|
2.2 |
Sheet weight |
5 |
||||
|
2.3 |
Water absorbability |
60 |
||||
|
2.4 |
Break-bending load |
50 |
||||
|
2.5 |
Water-proof duration |
20 |
||||
|
2.6 |
Volumetric weight |
50 |
||||
|
2.7 |
Appearance |
30 |
||||
|
3 |
Concrete |
|||||
|
3.1 |
Air content |
1 sample |
TCVN 3111:1993 |
80 |
||
|
3.2 |
Volumetric weight |
ditto |
TCVN 3115:1993 BS 1881:1983-P.114 ASTM C 642-97 |
30 30 30 |
||
|
3.3 |
Concretion duration |
ditto |
ASTM C 403-99 |
350 |
||
|
3.4 |
Slump |
ditto |
TCVN 3106:1993 |
20 |
||
|
3.5 |
Compression test on available samples |
3 samples |
TCVN 3118:1993 |
2 |
90 |
|
|
3.6 |
Bending strength of concrete |
3 samples |
TCVN 3119:1993 |
120 |
||
|
3.7 |
Water absorbability |
3 samples |
TCVN 3113:1993 |
60 |
||
|
3.8 |
Specific weight |
3 samples |
TCVN 3112:1993 |
30 |
||
|
3.9 |
Module of elasticity |
3 samples |
ASTM C 469-94 |
140 |
||
|
3.10 |
Concrete dry shrinkage, after 14 days |
3 samples |
ASTM C 157-99 |
300 |
||
|
3.11 |
Drilling for concrete sampling and compression test |
1 piece |
TCVN 3118: 1993 |
5 |
||
|
- Æ 75 |
500 |
|||||
|
- Æ 100 |
600 |
|||||
|
- Æ 150 |
800 |
|||||
|
3.12 |
Model molding at site and compression test in labs |
3 pieces |
TCVN 3105: 1993 TCVN 4453: 1995 |
200 |
Travel expenses not yet included 7, 28 days |
|
|
3.13 |
Aggregate concrete layout |
3 pieces |
400 |
|||
|
4 |
Concrete additives |
5 liters |
30 |
|||
|
4.1 |
Volumetric ratio |
ASTM C 494-99a |
50 |
|||
|
4.2 |
Post-drying remainder |
ASTM C 494-99 |
150 |
|||
|
4.3 |
Conformity with ASTM C 494 |
ASTM C 494-99a |
2,000 |
Material and testing expenses not yet included |
||
|
4.4 |
Conformity with BS 5075 |
BS 5075: 1985 |
2,000 |
|||
|
5 |
Colored cement flooring tiles |
20 pieces |
TCVN 6065:1995 |
6 |
||
|
5.1 |
Basic dimensions |
20 |
||||
|
5.2 |
Water absorbability |
60 |
||||
|
5.3 |
Shock-force resistance |
30 |
||||
|
5.4 |
Break-bending load on the whole tile |
80 |
||||
|
5.5 |
Tile weight |
10 |
||||
|
5.6 |
Abradability |
150 |
||||
|
6 |
Pipe culverts |
1 pipe |
AS 4058-1992 |
4 |
||
|
6.1 |
Basic dimensions |
40 |
||||
|
6.2 |
Water absorbability |
200 |
Method of sampling drilling |
|||
|
6.3 |
Cracking compressive force |
100 |
||||
|
6.4 |
Destroying compressive force |
100 |
||||
|
7 |
Centrifugal reinforced concrete electric posts |
1 pile |
3 |
|||
|
7.1 |
Basic dimensions |
TCVN 5847:1994 |
20 |
|||
|
7.2 |
Appearance |
TCVN 5847:1994 |
20 |
|||
|
7.3 |
Compression intensity of concrete |
20 TCN 162-87 |
80 |
|||
|
7.4 |
Post-tip tensile load test |
TCVN 5847:1994 |
250 |
|||
|
8 |
Sand, stone, gravel |
20 kg |
TCVN 1772:1987 TCVN 339:1986 TCVN 345:1986 |
7 |
||
|
8.1 |
Specific weight |
20 |
||||
|
8.2 |
Volumetric weight |
20 |
||||
|
8.3 |
Granular composition |
100 |
||||
|
8.4 |
Content of organic impurities |
20 |
||||
|
8.5 |
Content of flat diamond-shaped granules |
30 |
||||
|
8.6 |
Durability in sulfate environment |
ASTM C 88-99a |
300 |
|||
|
8.7 |
Porous volumetric weight |
20 |
||||
|
8.8 |
Moisture |
20 |
||||
|
8.9 |
Water absorbability |
60 |
||||
|
8.10 |
Compactness in cylinder |
80 |
||||
|
8.11 |
Compression strength limit (rubble) |
120 |
for one state |
|||
|
8.12 |
Content of dust, mud, soil |
20 |
||||
|
8.13 |
Abradability in trommel |
80 |
||||
|
9 |
Bitumen |
4 kg |
22 TCN 63-84 |
6 |
||
|
9.1 |
Softening temperature |
50 |
||||
|
9.2 |
Elongation |
80 |
||||
|
9.3 |
Adhesiveness strength of stone or concrete |
40 |
||||
|
9.4 |
Inflammable temperature |
60 |
||||
|
9.5 |
Settlement degree at |
50 |
||||
|
9.6 |
Specific weight |
40 |
||||
|
9.7 |
Lost quantity after heating at 168o C for 5 hours |
100 |
||||
|
10 |
Bituminous concrete |
3 pieces |
22 TCN 62-84 |
10 |
||
|
A. Bituminous concrete |
AASHTO T 245-90 |
Minimum sampling |
||||
|
10.1 |
Volumetric weight |
1 |
30 |
quantity of 15 pieces |
||
|
10.2 |
Water saturation |
1 |
30 |
D = 100 mm |
||
|
10.3 |
Expansion |
1 |
20 |
|||
|
10.4 |
Roller-compact density |
1 |
20 |
|||
|
10.5 |
Excessive porosity |
1 |
20 |
|||
|
10.6 |
Compression intensity at 20oC |
3 |
150 |
|||
|
10.6 |
Compression intensity at 60oC |
3 |
150 |
|||
|
10.7 |
Compression intensity in the saturation state |
3 |
150 |
|||
|
10.8 |
Compression intensity after 15 days of saturated immersion |
3 |
150 |
|||
|
10.9 |
Marshall durability |
3 |
300 |
|||
|
10.10 |
Marshall plasticity |
3 |
30 |
|||
|
10.11 |
Conventional hardness |
3 |
60 |
|||
|
10.12 |
Bituminous content |
1 |
100 |
|||
|
Total of part A |
1,180 |
|||||
|
B. Re-made samples (from part A�s ones) |
||||||
|
10.1 |
Volumetric weight after remaking |
1 |
30 |
|||
|
10.2 |
Compression intensity at 20oC |
3 |
150 |
|||
|
10.3 |
Compression intensity at 50oC |
3 |
150 |
|||
|
10.4 |
Compression intensity in the saturation state |
3 |
150 |
|||
|
10.5 |
Compression intensity after 15 days of saturated immersion |
3 |
150 |
|||
|
10.6 |
Marshall plasticity |
3 |
30 |
|||
|
10.7 |
Conventional hardness |
3 |
60 |
|||
|
10.8 |
Molded samples for experiment |
12 |
240 |
|||
|
Total of part B |
960 |
|||||
|
C. Hot bituminous concrete (unmolded models) |
30 kg |
|||||
|
Expenses for experiment shall be calculated as in Part A, plus expense for processing and molding samples for experiment as in Item 10.8, Part B |
1,420 |
|||||
|
11 |
Earth |
30 kg |
6 |
|||
|
11.1 |
Moisture |
TCVN 4196:1995 |
40 |
|||
|
11.2 |
Rolling limits |
TCVN 4197:1995 |
40 |
|||
|
11.3 |
Flowing limits |
TCVN 4197:1995 |
40 |
|||
|
11.4 |
Granular composition |
TCVN 4198:1986 |
150 |
|||
|
11.5 |
California Bearing Ratio (CBR) in laboratories |
ASTM D1883-94 |
600 |
|||
|
11.6 |
Test of standard compactness |
TCVN 4201:1995 |
300 |
|||
|
11.7 |
Shaping moisture |
TCVN 4344:1986 |
30 |
|||
|
11.8 |
Sensibility when drying |
TCVN 4345:1986 |
40 |
|||
|
11.9 |
Shrinkage when drying |
TCVN 4345:1986 |
50 |
|||
|
11.10 |
Tensile strength |
TCVN 4345:1986 |
100 |
|||
|
11.11 |
Water absorbability after baking |
TCVN 4345:1986 |
80 |
|||
|
11.12 |
Compression strength |
TCVN 4345:1986 |
100 |
|||
|
11.13 |
Plasticity |
TCVN 4345:1986 |
60 |
|||
|
11.14 |
Granular composition |
TCVN 4345:1986 |
140 |
|||
|
12 |
Building bricks |
25 pieces |
TCVN 6355:1998 |
6 |
||
|
12.1 |
Basic dimensions and |
|||||
|
appearance |
20 |
|||||
|
12.2 |
Compression strength |
90 |
||||
|
12.3 |
Flexural strength |
70 |
||||
|
12.4 |
Water absorbability |
60 |
||||
|
12.5 |
Specific weight |
30 |
||||
|
12.6 |
Volumetric weight |
10 |
||||
|
12.7 |
Porosity |
40 |
||||
|
12.8 |
Lime stain |
40 |
||||
|
12.9 |
Desalinity |
80 |
||||
|
13 |
Roofling tiles |
20 pieces |
TCVN 4313:1995 |
6 |
||
|
13.1 |
Basic dimensions |
20 |
||||
|
13.2 |
Water absorbability |
60 |
||||
|
13.3 |
Water-proof duration |
40 |
||||
|
13.4 |
Break-bending load |
|||||
|
on the whole tile |
80 |
|||||
|
13.5 |
Weight of 1 m2 of water-saturated roofing tile |
20 |
||||
|
14 |
Clay flooring tiles |
15 pieces |
TC 04-87 (Dong Nai Brick and Tile) |
6 |
||
|
14.1 |
Basic dimensions |
20 |
||||
|
14.2 |
Water absorbability |
60 |
||||
|
14.3 |
Flexural strength |
80 |
||||
|
15 |
Decoration tiles |
15 pieces |
TC 04-87 (Dong Nai Brick and Tile) |
6 |
||
|
15.1 |
Basic dimensions |
20 |
||||
|
15.2 |
Water absorbability |
60 |
||||
|
15.3 |
Compression strength |
80 |
||||
|
16 |
Flooring glazed tiles wall-covering glazed tiles |
60 pieces |
TCVN 6415:1998 |
20 |
||
|
16.1 |
Basic dimensions |
10 pieces |
30 |
|||
|
16.2 |
Water absorbability |
20 pieces |
60 |
|||
|
16.3 |
Flexural strength limit |
20 pieces |
130 |
|||
|
16.4 |
Heat-shock strength |
20 pieces |
100 |
|||
|
16.5 |
Thermo-stability |
10 pieces |
100 |
|||
|
16.6 |
Chemico-stability |
10 pieces |
150 |
|||
|
16.7 |
Mohs hardness |
10 pieces |
40 |
|||
|
16.8 |
Surface abradability |
10 pieces |
350 |
|||
|
16.9 |
Appearance |
10 pieces |
50 |
|||
|
17 |
Porcelain sanitary ware |
1 piece |
6 |
|||
|
17.1 |
Water-absorbability |
TCVN 5436:1986 |
60 |
|||
|
17.2 |
Thermo-stability |
TCVN 5437:1986 |
40 |
|||
|
17.3 |
Compression strength |
TCVN 5436:1986 |
80 |
|||
|
18 |
Fire bricks |
5 pieces |
TCVN 176:1986 |
6 |
||
|
18.1 |
Basic dimensions |
20 |
||||
|
18.2 |
Apparent porosity |
30 |
||||
|
18.3 |
Volumetric weight |
30 |
||||
|
18.4 |
Compression strength |
100 |
||||
|
19 |
Wood |
5 bars |
7 |
3 x 5 x 10 cm |
||
|
19.1 |
Moisture |
TCVN 358:1970 |
30 |
|||
|
19.2 |
Volumetric weight |
TCVN 369:1970 |
20 |
|||
|
19.3 |
Tensile strength limit |
TCVN 364:1970 |
80 |
|||
|
19.4 |
Flexural strength limit |
TCVN 365:1970 |
80 |
|||
|
19.5 |
Compression strength limit |
TCVN 363:1970 |
80 |
|||
|
19.6 |
Hardness |
TCVN 369:1970 |
70 |
|||
|
19.7 |
Elongation or shrinkage |
TCVN 360:1970 |
40 |
|||
|
20 |
Wood products |
1 m2 |
TC 04-90 (Dong Nai Wood Furniture) |
5 |
||
|
20.1 |
Varnished surface-breaking strength |
80 |
||||
|
20.2 |
Moisture |
25 |
||||
|
20.3 |
Dilatancy |
20 |
||||
|
20.4 |
Water absorbability |
20 |
||||
|
20.5 |
Thermo-stability |
40 |
||||
|
21 |
Inspection of concrete quality at project sites |
|||||
|
21.1 |
Checking concrete degree with bouncing gun, for each member the test shall be made on at least 3 sections, 10 points on each section |
130 |
||||
|
21.2 |
Combination of the above-said two methods for one member |
270 |
||||
|
21.3 |
Use of ultrasound to determine the reinforcement�s position and diameter |
550 |
DOMAIN: ELECTRICITY
|
Ordinal number |
Product names - criteria |
Quantity |
Testing method |
Duration day |
Unit price VND 1,000 |
Notes |
|
1 |
Home electric appliances |
3 samples |
TCVN 5699-1:98 IEC 335-1 |
7 |
||
|
1.1 |
Classification |
20 |
||||
|
1.2 |
Labeling and instructions (21 parts) |
100 |
||||
|
1.3 |
Protection against incidental contact with electrified parts |
60 |
||||
|
1.4 |
Starting of transmission apparatuses by electric motors |
50 |
||||
|
1.5 |
Electric output and current |
70 |
||||
|
1.6 |
Heating In normal operation state |
80 |
for one state |
|||
|
1.7 |
Leaked current and electro- stability at working temperature |
70 |
||||
|
1.8 |
Moisture test |
300 |
for one cycle |
|||
|
1.9 |
Leaked current and electro- stability |
40 |
||||
|
1.10 |
Testing of abnormal manipulations |
100 |
for one state |
|||
|
1.11 |
Mechanical stability and danger |
50 |
||||
|
1.12 |
Mechanical durability |
50 |
||||
|
1.13 |
Structure |
|
||||
|
Protection grades of IP 5X to IP 6X |
400 |
|||||
|
Structural requirements (42 parts) |
200 |
|||||
|
1.14 |
Inner conductor (9 parts) |
80 |
||||
|
1.15 |
Supplementary accessories (10 parts) |
80 |
||||
|
1.16 |
Source connector and soft outer conductor (27 parts) |
200 |
||||
|
1.17 |
Connector used for outer conductor (12 parts) |
150 |
||||
|
1.18 |
Earthing line (5 parts) |
80 |
||||
|
1.19 |
Screw and splice (4 parts) |
60 |
||||
|
1.20 |
Leakage length and insulation clearing |
60 |
||||
|
1.21 |
Heat- and fire-resistance and surface discharge (7 parts) |
- 300 |
||||
|
2 |
Electric wire and cable |
|||||
|
2.1 |
Plastic-covered wire |
10m |
TCVN 2103 : 1994 |
5 |
||
|
2.1 |
Structure and signs |
20 |
||||
|
2.2 |
Fiber cross-section diameter |
20 |
per core |
|||
|
2.3 |
Overall diameter |
20 |
per core |
|||
|
2.4 |
Number of wires |
10 |
||||
|
2.5 |
Cross-section |
30 |
||||
|
2.6 |
Outer diameter |
20 |
||||
|
2.7 |
Insulation thickness |
20 |
per core |
|||
|
2.8 |
Conductor quality |
10 |
||||
|
2.9 |
Cover quality |
10 |
||||
|
2.10 |
Conductor traction limit ratio |
30 |
one per core |
|||
|
2.11 |
Relative elongation of conductor |
20 |
per core |
|||
|
2.12 |
DC resistance at 20o C |
20 |
per core |
|||
|
2.13 |
Insulation resistance at 20o C and 70oC |
40 |
each temperature |
|||
|
2.14 |
Test of tension standing |
40 |
||||
|
2.15 |
Self-combustibility of insulator |
20 |
||||
|
2.16 |
Ageing test |
50 |
by days |
|||
|
2.17 |
Traction strength of cover, insulator |
40 |
one core |
|||
|
2.18 |
Elongation of cover, insulator |
20 |
one core |
|||
|
2.19 |
Insulation shrinkage |
30 |
one core |
|||
|
2.20 |
Insulation deformity |
30 |
one core |
|||
|
2.21 |
Insulation heat-resistance |
50 |
one core |
|||
|
2.22 |
Crack-proof of insulation and cover |
40 |
||||
|
3 |
PVF electro-magnetic wire |
50 m |
TCVN 4305:1992 |
5 |
||
|
3.1 |
Dimensions |
20 |
||||
|
3.2 |
DC resistance |
40 |
||||
|
3.3 |
Relative elongation |
30 |
||||
|
3.4 |
Plasticity |
80 |
||||
|
3.5 |
Adhesiveness |
50 |
||||
|
3.6 |
Abrasion-proof |
50 |
||||
|
3.7 |
Flexibility |
80 |
||||
|
3.8 |
Electro-stability |
30 |
||||
|
3.9 |
Heat impulse-resistance |
50 |
||||
|
4 |
Pew electro-magnetic wire |
50 m |
TCVN 6337:1998 |
5 |
||
|
4.1 |
Dimensions |
20 |
||||
|
4.2 |
DC resistance |
40 |
||||
|
4.3 |
Relative elongation |
30 |
||||
|
4.4 |
Plasticity and adhesiveness |
40 |
||||
|
4.5 |
Heat impulse-resistance |
50 |
||||
|
4.6 |
Electro-stability |
80 |
||||
|
4.7 |
Cavity |
50 |
||||
|
4.8 |
Abrasion-proof |
50 |
||||
|
4.9 |
Elasticity |
80 |
||||
|
5 |
Electric cable |
12 m |
TCVN 5935:1995 |
14 |
||
|
5.1 |
Conductor structure |
30 |
||||
|
5.2 |
Diameter of conducting wire |
20 |
per core |
|||
|
5.3 |
Mechanical durability of conducting wire |
80 |
three cores |
|||
|
5.4 |
DC resistance of conductor |
70 |
three cores |
|||
|
5.5 |
Test of local discharge |
300 |
one per core |
|||
|
5.6 |
Flexural test combined with local discharge test |
350 |
one per core |
|||
|
5.7 |
Intake power coefficient d |
250 |
per core |
|||
|
5.8 |
Thermo-cycle test combined with local discharge test |
250 |
one per cycle |
|||
|
5.9 |
Impulse test combined with voltage-standing test |
250 |
one per core |
|||
|
5.10 |
Voltage-standing test |
|||||
|
- In 5 minutes |
50 |
|||||
|
- In 4 hours |
200 |
|||||
|
5.11 |
Block resistivity of insulator |
at 20o C, 70o C or 90o C |
80 |
two states |
||
|
5.12 |
Insulation thickness |
20 |
per core |
|||
|
5.13 |
Mechanical durability of insulator |
80 |
one per core |
|||
|
5.14 |
Insulator ageing test |
40 |
per day |
|||
|
5.15 |
Heat test |
60 |
per core |
|||
|
5.16 |
Crack-proof test of insulator |
40 |
per core |
|||
|
5.17 |
Water-absorbability test of insulator |
500 |
||||
|
5.18 |
Compression test at high temperature for insulator |
120 |
three per core |
|||
|
5.19 |
Shrinkage test for insulator |
30 |
one per core |
|||
|
5.20 |
Cover thickness |
20 |
||||
|
5.21 |
Mechanical durability of cover |
80 |
one per core |
|||
|
5.22 |
Cover ageing test |
30 |
per one per day |
|||
|
5.23 |
Cover crack-proof test |
30 |
||||
|
5.24 |
Cover weight loss |
250 |
||||
|
5.25 |
Compression test at high temperatures for cover |
120 |
three per core |
|||
|
5.26 |
Fire test |
50 |
||||
|
5.27 |
Ageing test on complete cable samples |
30 |
one per day |
|||
|
5.28 |
Tensile strength of conductor |
100 |
three per core |
|||
|
6 |
Low-voltage electric instruments |
|||||
|
6.1 |
Automatic circuit breaker |
1-15 |
TCVN 6434:1998 |
10 |
||
|
6.1.1 |
Fadelessness of labels |
50 |
||||
|
6.1.2 |
Reliability of screw, conducting parts and connectors |
50 |
||||
|
6.1.3 |
Reliability of connectors used for outer conductor |
50 |
||||
|
6.1.4 |
Protection against electric shock |
20 |
||||
|
6.1.5 |
Dielectric property |
150 |
||||
|
6.1.6 |
Heating |
100 |
||||
|
6.1.7 |
28-day test |
200 |
per cycle |
|||
|
6.1.8 |
Impact property |
50 |
one per mode |
|||
|
6.1.9 |
Heat-resistance |
80 |
||||
|
6.1.10 |
Abnormal heat- and fire-resitance |
180 |
||||
|
6.1.11 |
Anti-rust durability |
50 |
||||
|
7 |
Other electric products |
|||||
|
7.1 |
Ballast used for fluorescent tubes |
1-5 |
TCVN 6478:1999 |
45 |
||
|
7.1.1 |
Classification |
20 |
||||
|
7.1.2 |
Labeling and instruction |
100 |
||||
|
7.1.3 |
Protection against incidental contact with electrified parts |
30 |
||||
|
7.1.4 |
Connectors |
100 |
||||
|
7.1.5 |
Earthing requirements |
100 |
||||
|
7.1.6 |
Moisture-resistance and insulation |
150 |
||||
|
7.1.7 |
Thermal stability of coil |
1,500 |
||||
|
7.1.8 |
Ballast heating |
140 |
per mode |
|||
|
7.1.9 |
Screw, current conductor and splice |
100 |
||||
|
7.1.10 |
Length of leak and air gap |
60 |
||||
|
7.1.11 |
Heat- and fire-resistance |
180 |
||||
|
7.1.12 |
Anti-rust quality |
50 |
||||
|
7.2 |
Ballast used for fluorescent lamps |
1-5 |
TCVN 6479:1999 |
7 |
||
|
7.2.1 |
Labeling |
50 |
||||
|
7.2.2 |
Open-circuited voltage at lamp connector or starter |
30 |
||||
|
7.2.3 |
Pre-heating condition |
50 |
||||
|
7.2.4 |
Electric output and current on lamp |
50 |
||||
|
7.2.5 |
Circuit output coefficient |
30 |
||||
|
7.2.6 |
Supply electric current |
30 |
||||
|
7.2.7 |
Magnetic field screen |
30 |
||||
|
7.3 |
Lamps |
5-10 |
IEC 60598-1 (1992) |
20 |
||
|
7.3.1 |
Labeling |
80 |
||||
|
7.3.2 |
Structure |
120 |
||||
|
7.3.3 |
Inner and outer conductors |
150 |
||||
|
7.3.4 |
Earthing requirements |
80 |
||||
|
7.3.5 |
Protection against electric shock |
80 |
||||
|
7.3.6 |
Protection against dust, hard objects and moisture |
50 |
IP1X-IP4X |
|||
|
7.3.7 |
Insulation resistance and electric strength |
80 |
||||
|
7.3.8 |
Length of leak and air gap |
60 |
||||
|
7.3.9 |
Durability and thermal stability |
100 |
per mode |
|||
|
7.3.10 |
Heat- and fire-resistance and surface discharge |
300 |
||||
|
7.3.11 |
Screwed connector |
150 |
||||
|
7.3.12 |
Connector without screw and splice |
150 |